Score line corrosion protection for container end walls
    1.
    发明申请
    Score line corrosion protection for container end walls 审中-公开
    容器端壁刻痕线防腐蚀

    公开(公告)号:US20100227191A1

    公开(公告)日:2010-09-09

    申请号:US12657876

    申请日:2010-01-28

    IPC分类号: B32B1/08 B32B15/01 B32B15/20

    摘要: The invention relates to an end wall of a metal container having a score therein. The end wall is made of a composite metal sheet made of two or more metal layers, one of the layers being made of an aluminum alloy of high strength (e.g. a high magnesium alloy such as AA5182, AA5042 or AA5082, optionally with increased Mg), and another of the layers being made of an aluminum alloy having a good resistance to stress corrosion cracking (e.g. aluminum alloys AA3004, AA3104, AA5006 or AA5005), wherein at least the bottom of the score is formed by a surface of the alloy of good resistance to stress corrosion cracking.

    摘要翻译: 本发明涉及一种具有分数的金属容器的端壁。 端壁由两层或多层金属层制成的复合金属板制成,其中一层由高强度的铝合金制成(如高镁合金如AA5182,AA5042或AA5082,任选含有增加的Mg) ,另一个层由具有良好的耐应力腐蚀开裂性的铝合金(例如铝合金AA3004,AA3104,AA5006或AA5005)制成,其中至少该刻痕的底部由 良好的抗应力腐蚀开裂性能。