公开(公告)号:US4207296A
公开(公告)日:1980-06-10
申请号:US942835
申请日:1978-09-15
申请人: Harry H. K. Nauta , Jan W. Kok , Jan Harte
发明人: Harry H. K. Nauta , Jan W. Kok , Jan Harte
CPC分类号: C01G39/02 , C01G39/00 , C01P2006/80
摘要: Molybdenum trioxide containing potassium is heated to a temperature sufficiently high (i.e. at least about 525.degree. C.) to render the potassium soluble in hot water, the heated trioxide is quenched to less than about 400.degree. C. at a rate of at least about 30.degree. C. per minute, the quenched trioxide is leached with hot water (between about 50.degree. C. and about 100.degree. C.) to leach the solubilized potassium and after liquid-solids separation the molybdenum trioxide is dissolved in ammonium hydroxide to form ammonium molybdates, which can be recovered from solution and then can be calcined to chemical grade molybdic oxide. The process is advantageously conducted in conjunction with the roasting of molybdenite.
摘要翻译: 将含有三氧化钼的钾加热到足够高的温度(即至少约525℃)以使钾溶于热水中,将加热的三氧化二砷以至少约 每分钟30℃,用热水(约50℃至约100℃)浸泡淬灭的三氧化硫以浸出溶解的钾,并且在液固固体分离后,将三氧化钼溶解在氢氧化铵中形成 钼酸铵,可从溶液中回收,然后煅烧成化学级的氧化钼。 该方法有利地与辉钼矿的焙烧结合进行。