METHOD FOR MANUFACTURING DYED WOVEN OR KNITTED FABRIC USING METALLIC YARN AND POLYESTER YARN AND FABRIC MANUFACTURED USING THE METHOD
    1.
    发明申请
    METHOD FOR MANUFACTURING DYED WOVEN OR KNITTED FABRIC USING METALLIC YARN AND POLYESTER YARN AND FABRIC MANUFACTURED USING THE METHOD 审中-公开
    使用金属纱线和聚酯纱线制造染色的织造或编织织物的方法和使用该方法制造的织物

    公开(公告)号:US20140310889A1

    公开(公告)日:2014-10-23

    申请号:US14358034

    申请日:2012-05-30

    CPC classification number: D06P1/0008 D06P1/008 D06P3/34 D06P3/52 D06P3/80 D06P3/82

    Abstract: A method for manufacturing dyed woven or knitted fabric includes preparing woven or knitted fabric using metallic yarn and normal-pressure dyeing polyester yarn having an elasticity modulus of 400 to 600 kg/mm2 and an elongation of 30 to 40%, fabricating a dye bath by putting a dye solution obtained by dispersing a dye in water, dyeing the woven or knitted fabric by putting the prepared woven or knitted fabric into the fabricated dye bath, raising a temperature of the dye bath starting from 35 to 45° C. for 30 to 50 minutes at a rate of 1.2 to 1.5° C./min, and maintaining the heated dye bath at 90 to 100° C. for 15 to 25 minutes, and washing the dyed woven or knitted fabric. The dyed woven or knitted fabric has a light reflection reduction rate of 20% to 30%.

    Abstract translation: 制造染色机织或编织物的方法包括使用金属丝和弹性模量为400至600kg / mm 2和伸长率为30至40%的常压染色涤纶纱线制备编织物或针织物,制造染浴 将通过将染料分散在水中而获得的染料溶液,通过将制备的编织物或针织物放入制造的染浴中对织造或针织物进行染色,将染浴从35℃开始升温至30℃至30℃ 50分钟,速率为1.2〜1.5℃/分钟,并将加热的染浴保持在90〜100℃15〜25分钟,洗涤染色机织或针织物。 染色机织或针织物的光反射减少率为20%至30%。