Conductive titanium oxide comprising titanium oxide of columnar shape and specific dimensions, and processes for producing thereof
    1.
    发明授权
    Conductive titanium oxide comprising titanium oxide of columnar shape and specific dimensions, and processes for producing thereof 有权
    包含柱状和特定尺寸的氧化钛的导电性氧化钛及其制造方法

    公开(公告)号:US08227083B2

    公开(公告)日:2012-07-24

    申请号:US12224812

    申请日:2007-03-06

    摘要: Titanium dioxide and an electro-conductive titanium oxide which each includes particles having a large major-axis length in a large proportion and comprises columnar particles having a satisfactory particle size distribution. A titanium compound, an alkali metal compound, and an oxyphosphorus compound are heated/fired in the presence of titanium dioxide nucleus crystals having an aspect ratio of 2 or higher to grow the titanium dioxide nucleus crystals. Subsequently, a titanium compound, an alkali metal compound, and an oxyphosphorus compound are further added and heated/fired in the presence of the grown titanium dioxide nucleus crystals. Thus, titanium dioxide is produced which comprises columnar particles having a weight-average major-axis length of 7.0-15.0 μm and in which particles having a major-axis length of 10 μm or longer account for 15 wt. % or more of all the particles. A solution of a tin compound and a solution of compounds of antimony, phosphorus, etc. are added to a suspension obtained by suspending the titanium dioxide. The particles are sedimented. Subsequently, the product obtained is heated/fired to produce an electro-conductive titanium oxide which comprises the titanium dioxide and an electro-conductive coating formed on the surface thereof.

    摘要翻译: 二氧化钛和导电性氧化钛,其各自包括大比例的长轴长度大的颗粒,并且包括具有令人满意的粒度分布的柱状颗粒。 在长宽比为2以上的二氧化钛核晶体的存在下,对钛化合物,碱金属化合物和氧磷化合物进行加热烧成,生长二氧化钛核晶体。 随后,在生长的二氧化钛核晶体的存在下,进一步添加钛化合物,碱金属化合物和氧磷化合物并加热/烧制。 因此,制造二氧化钛,其包括重均长轴长度为7.0-15.0μm的柱状颗粒,其中长轴长度为10μm或更大的颗粒占15重量%。 所有颗粒的百分比或更多。 将锡化合物和锑,磷等化合物的溶液加入到通过悬浮二氧化钛获得的悬浮液中。 颗粒沉淀。 随后,将获得的产物加热/烧制以制备包含二氧化钛的导电氧化钛和在其表面上形成的导电涂层。

    Black resin composition for display device, and member for display device
    4.
    发明授权
    Black resin composition for display device, and member for display device 有权
    用于显示装置的黑色树脂组合物和用于显示装置的构件

    公开(公告)号:US07785501B2

    公开(公告)日:2010-08-31

    申请号:US11722002

    申请日:2005-12-27

    IPC分类号: H01B1/06 G02B5/20

    摘要: A black resin composition for a display device, which can achieve a high optical density even when its light-blocking agent content is relatively low and can achieve a high optical density even when it is formed into a thin film, and a member for display device which can reduce unevenness of display caused by a level difference in a pixel part resulting from the film thickness of the black resin composition. The black resin composition for a display device has a black titanium oxynitride represented by composition formula: TiNxOy-nSiO2 (wherein x and y each are a real number of larger than 0 but less than 2, and n is a real number within the range of 0 less than or equal to n less than or equal to 0.05), containing a nitrogen atom represented by N in an amount of 17 wt % or more but less than 23 wt %, and having a specific surface area of 5 to 30 m2/g and a crystalline size as measured with an X-ray diffractometer of 17 to 25 nm, and a curable binder system. Also, a member for display device having a light-blocking layer formed using the said black resin composition for display device.

    摘要翻译: 一种用于显示装置的黑色树脂组合物,即使其遮光剂含量相对较低也能够获得高的光密度,并且即使形成为薄膜也可以实现高的光密度,以及显示装置的构件 这可以减少由黑色树脂组合物的膜厚度导致的像素部分的电平差引起的显示不均匀。 用于显示装置的黑色树脂组合物具有由组成式:TiN x O y-n SiO 2(其中x和y各自是大于0但小于2的实数)表示的黑色氮氧化钛,并且n是在 0以下,n小于或等于0.05),含有由17重量%以上且小于23重量%的N表示的氮原子,比表面积为5〜30m 2 / g和用17至25nm的X射线衍射仪测量的结晶尺寸和可固化粘合剂体系。 而且,具有使用该显示装置用黑色树脂组合物形成的遮光层的显示装置用部件。

    Black Resin Composition for Display Device, and Member for Display Device
    6.
    发明申请
    Black Resin Composition for Display Device, and Member for Display Device 有权
    用于显示装置的黑色树脂组合物和显示装置的构件

    公开(公告)号:US20080318018A1

    公开(公告)日:2008-12-25

    申请号:US11722002

    申请日:2005-12-27

    IPC分类号: B32B27/00

    摘要: A black resin composition for a display device, which can achieve a high optical density even when its light-blocking agent content is relatively low and can achieve a high optical density even when it is formed into a thin film, and a member for display device which can reduce unevenness of display caused by a level difference in a pixel part resulting from the film thickness of the black resin composition. The black resin composition for a display device has a black titanium oxynitride represented by composition formula: TiNxOy-nSiO2 (wherein x and y each are a real number of larger than 0 but less than 2, and n is a real number within the range of 0≦n≦0.05), containing a nitrogen atom represented by N in an amount of 17 wt % or more but less than 23 wt %, and having a specific surface area of 5 to 30 m2/g and a crystalline size as measured with an X-ray diffractometer of 17 to 25 nm, and a curable binder system. Also, a member for display device having a light-blocking layer formed using the said black resin composition for display device.

    摘要翻译: 一种用于显示装置的黑色树脂组合物,即使其遮光剂含量相对较低也能够获得高的光密度,并且即使形成为薄膜也可以实现高的光密度,以及显示装置的构件 这可以减少由黑色树脂组合物的膜厚度导致的像素部分的电平差引起的显示不均匀。 用于显示装置的黑色树脂组合物具有由组成式:TiN x O y-n SiO 2(其中x和y各自是大于0但小于2的实数)表示的黑色氮氧化钛,并且n是在 0≤n≤0.05),含有17重量%以上且小于23重量%的N表示的氮原子,比表面积为5〜30m 2 / g,结晶尺寸为 用17至25nm的X射线衍射仪测量,和可固化的粘合剂体系。 而且,具有使用该显示装置用黑色树脂组合物形成的遮光层的显示装置用部件。

    Titanium Oxide, Conductive Titanium Oxide, and Processes for Producing These
    9.
    发明申请
    Titanium Oxide, Conductive Titanium Oxide, and Processes for Producing These 有权
    氧化钛,导电氧化钛及其生产工艺

    公开(公告)号:US20090117383A1

    公开(公告)日:2009-05-07

    申请号:US12224812

    申请日:2007-03-06

    摘要: Titanium dioxide and an electro-conductive titanium oxide which each includes particles having a large major-axis length in a large proportion and comprises columnar particles having a satisfactory particle size distribution. A titanium compound, an alkali metal compound, and an oxyphosphorus compound are heated/fired in the presence of titanium dioxide nucleus crystals having an aspect ratio of 2 or higher to grow the titanium dioxide nucleus crystals. Subsequently, a titanium compound, an alkali metal compound, and an oxyphosphorus compound are further added and heated/fired in the presence of the grown titanium dioxide nucleus crystals. Thus, titanium dioxide is produced which comprises columnar particles having a weight-average major-axis length of 7.0-15.0 μm and in which particles having a major-axis length of 10 μm or longer account for 15 wt. % or more of all the particles. A solution of a tin compound and a solution of compounds of antimony, phosphorus, etc. are added to a suspension obtained by suspending the titanium dioxide. The particles are sedimented. Subsequently, the product obtained is heated/fired to produce an electro-conductive titanium oxide which comprises the titanium dioxide and an electro-conductive coating formed on the surface thereof.

    摘要翻译: 二氧化钛和导电性氧化钛,其各自包括大比例的长轴长度大的颗粒,并且包括具有令人满意的粒度分布的柱状颗粒。 在长宽比为2以上的二氧化钛核晶体的存在下,对钛化合物,碱金属化合物和氧磷化合物进行加热烧成,生长二氧化钛核晶体。 随后,在生长的二氧化钛核晶体的存在下,进一步添加钛化合物,碱金属化合物和氧磷化合物并加热/烧制。 因此,生产二氧化钛,其包括重均长轴长度为7.0-15.0μm的柱状颗粒,其中长轴长度为10μm或更长的颗粒占15wt。 所有颗粒的百分比或更多。 将锡化合物和锑,磷等化合物的溶液加入到通过悬浮二氧化钛获得的悬浮液中。 颗粒沉淀。 随后,将获得的产物加热/烧制以制备包含二氧化钛的导电氧化钛和在其表面上形成的导电涂层。