摘要:
The present invention relates to a thermoplastic resin composition comprising 20 to 60 parts by weight of a rubber-reinforced resin (A) and 80 to 40 parts by weight of an aromatic polycarbonate (B) having an average molecular weight of 16,000 to 30,000 ((A)+(B)=100 parts by weight), said rubber-reinforced resin (A) containing a grafted rubber-like polymer (A1) obtained by polymerizing at least one compound (b) selected from the group consisting of aromatic vinyl compounds, vinyl cyanide compounds, (meth)acrylic ester compounds, acid anhydride monomeric compounds and maleimide-based compounds in the presence of a rubber-like polymer (a) having a glass transition temperature of not more than −40° C., the content of the rubber-like polymer (a) in the rubber-reinforced resin (A) being 10 to 70% by weight, and the grafted rubber-like polymer (A1) having such a particle size distribution that the weight percentage of the particles having a size of not less than 80 nm and less than 200 nm is not less than 30%, the weight percentage of the particles having a size of not less than 200 nm and less than 350 nm is not more than 70%, and the weight percentage of the particles having a size of not less than 350 nm is not more than 15%.
摘要:
Thermoplastic resin compositions containing a rubber-reinforced thermoplastic resin (A) obtained by graft polymerizing a monomeric mixture (b) in the presence of a rubber-like polymer (a), and a copolymer (B) obtained by polymerizing an aromatic vinyl compound, a vinyl cyanide compound and optionally other copolymerizable monomeric compound(s), which copolymer (B) being a mixture of a copolymer (B1) having Mw of 50,000 to 110,000 and a copolymer (B2) having Mw of 115,000 to 400,000. The content of the rubber-like polymer (a) content in the rubber-reinforced thermoplastic resin (A) is 10 to 25% by weight, the vinyl cyanide monomeric unit in the acetone soluble matter is 15 to 40% by weight, and the ratios of Mw to Mn and MZ to Mn of the acetone soluble matter being 2 to 5 and 5 to 11, respectively.
摘要翻译:含有通过在橡胶状聚合物(a)的存在下将单体混合物(b)接枝聚合得到的橡胶强化热塑性树脂(A)的热塑性树脂组合物和通过使芳香族乙烯基化合物聚合得到的共聚物(B) 乙烯基氰化合物和任选的其它可共聚的单体化合物,该共聚物(B)是具有50,000至110,000的M 的共聚物(B1)和具有M 小于115,000至400,000。 橡胶强化热塑性树脂(A)中的橡胶状聚合物(a)的含量为10〜25重量%,丙酮可溶物中的乙烯基氰单体单元为15〜40重量% 丙酮可溶物质的Mw与M N n和M Z至M n N的比值分别为2至5和5至11。
摘要:
A thermoplastic resin composition obtained by graft-polymerizing 95 to 50 parts by weight of a monomer mixture comprising a vinyl aromatic compound monomer and an acrylic compound monomer and optionally a vinyl cyanide compound monomer in the presence of 5 to 50 parts by weight of a rubbery substance consisting of styrene-butadiene copolymers, characterized in that the rubbery substance comprises (A) 40 to 80% by weight of a styrene-butadiene copolymer having a number-average particle diameter of at least 0.05 .mu.m and less than 0.2 .mu.m, a gel content of 30 to 100% by weight and a bound styrene content of 10 to 40% by weight and (B) 60 to 20% by weight of a styrene-butadiene copolymer having a number-average particle diameter of 0.2 to 3 .mu.m, a gel content of 10 to 80% by weight and a bound styrene content of 10 to 40% by weight and the total content of the components (A) and (B) in the rubbery substance is at least 80% by weight. Said thermoplastic resin composition is superior in chemical resistance, transparency, impact resistance and product appearance.
摘要:
A process for producing a polyorganosiloxane-based thermoplastic resin which comprises graft polymerizing (3) at least one vinyl monomer using (4) an initiator which is an organic peroxide which, upon decomposition, produces an organic radical represented by the structural formula: ##STR1## wherein R.sup.2, R.sup.3 and R.sup.4 represent independently hydrogen atoms or alkyl groups having 1 to 10 carbon atoms, in the presence of (2) a polyorganosiloxane.