公开(公告)号:US5374323A
公开(公告)日:1994-12-20
申请号:US750127
申请日:1991-08-26
申请人: G. William Kuhlman , Richard A. Beaumont , Daniel F. Carbaugh , David Anderson , Al Farrell , Amiya K. Chakrabarti , Kenneth P. Kinnear
发明人: G. William Kuhlman , Richard A. Beaumont , Daniel F. Carbaugh , David Anderson , Al Farrell , Amiya K. Chakrabarti , Kenneth P. Kinnear
摘要: Disclosed is a large alloy forging, the forging having an alloy composition selected from one of a nickel base alloy, a cobalt-chromium-nickel base alloy, a nickel-cobalt base alloy and an iron-nickel-chromium-molybdenum alloy, the forging having a grain size of ASTM grain size 3 or finer, as measured by ASTM method E112 and having a tensile strength in the range of 135 to 175 KSI.
摘要翻译: 公开了一种大型合金锻造,所述锻造具有选自镍基合金,钴 - 铬 - 镍基合金,镍 - 钴基合金和铁 - 镍 - 铬 - 钼合金之一的合金组成,所述锻造 具有ASTM晶粒尺寸3或更细的颗粒尺寸,通过ASTM方法E112测量并具有在135至175KSI范围内的拉伸强度。
-
公开(公告)号:US5360496A
公开(公告)日:1994-11-01
申请号:US44336
申请日:1993-04-07
申请人: G. William Kuhlman , Richard A. Beaumont , Daniel F. Carbaugh , David Anderson , Amiya K. Chakrabarti , Kenneth P. Kinnear
发明人: G. William Kuhlman , Richard A. Beaumont , Daniel F. Carbaugh , David Anderson , Amiya K. Chakrabarti , Kenneth P. Kinnear
摘要: Disclosed is a large alloy forging and method for making it. The forging having an alloy composition selected from one of a nickel base alloy, a cobalt-chromium-nickel base alloy, a nickel-cobalt base alloy and an iron-nickel-chromium-molybdenum alloy and having a grain size of ASTM grain size 4 or finer, as measured by ASTM method E112 and having a tensile strength in the range of 135 to 175 KSI. The process includes: (1) four upset forgings, (2) a rapid cooling after the final upset cooling, (3) a first and second upset forging with a reduction greater than 50%, (4) a third upset forging with a reduction greater than 25.%, and (5) a forging process with a fourth upset forging with a reduction greater than 50%.
摘要翻译: 公开了一种大型合金锻造及其制造方法。 具有选自镍基合金,钴 - 铬 - 镍基合金,镍 - 钴基合金和铁 - 镍 - 铬 - 钼合金之一并且具有ASTM晶粒尺寸4的晶粒尺寸的合金组成的锻造 或更细,如通过ASTM方法E112测量并且具有在135至175KSI范围内的拉伸强度。 该过程包括:(1)四个镦锻锻件,(2)最终镦锻冷却后的快速冷却,(3)第一和第二镦锻,压下率大于50%,(4) 大于25%,以及(5)锻造过程中,第四次锻造具有大于50%的压下率。
-