Polypropylenes having a reduced tendency to white fracture
    1.
    发明授权
    Polypropylenes having a reduced tendency to white fracture 失效
    具有降低白色断裂倾向的聚丙烯

    公开(公告)号:US5686533A

    公开(公告)日:1997-11-11

    申请号:US733017

    申请日:1996-10-16

    CPC分类号: C08L23/10 C08L2205/02

    摘要: Polypropylenes having a reduced tendency to white fracture, which contain A) from 70 to 95% by weight of a highly isotactic polypropylene having anisotactic index of more than 90 and a melt flow index between 0.1 and 100 g/10 min, it being possible for the polypropylene to be a homopolymer of propylene or a copolymer of propylene with one or more .alpha.-olefins, having a propylene content of at least 50 mol %, and B) from 5 to 30% by weight of a highly amorphous polypropylene having a crystalline polypropylene fraction of up to 10% by weight with an enthalpy of fusion of not more than 40 J/g and a melt flow index between 0.1 and 100 g/10 min, it being possible for the polypropylene to be a homopolymer of propylene or a copolymer of propylene with one or more .alpha.-olefins, having a propylene content of at least 80 mol %.

    摘要翻译: 具有降低的白色断裂倾向的聚丙烯,其含有A)70至95重量%的具有大于90的各向异性指数和0.1至100g / 10分钟的熔体流动指数的高度全同立构聚丙烯, 丙烯的均聚物或丙烯与一种或多种丙烯含量至少为50摩尔%的α-烯烃的共聚物的聚丙烯,和B)5-30重量%的具有结晶的高度无定形的聚丙烯 聚丙烯分数高达10重量%,熔融焓不超过40J / g,熔体流动指数为0.1-100g / 10min,聚丙烯可以是丙烯均聚物或 丙烯与一种或多种α-烯烃的共聚物,丙烯含量为至少80摩尔%。