3.
公开(公告)号:US4252867A
公开(公告)日:1981-02-24
申请号:US942190
申请日:1978-09-14
申请人: Keiji Nemoto , Kyoji Takahashi , Hiroyuki Hayashi
发明人: Keiji Nemoto , Kyoji Takahashi , Hiroyuki Hayashi
CPC分类号: C23C24/106 , Y10T428/12806 , Y10T428/12951
摘要: A corrosion-resistant iron-base material coated on at least a part of the surface thereof with a layer of a titanium-nickel alloy containing 5-45% by weight of nickel. This corrosion-resistant iron-base material is produced by applying a viscous coating liquid containing titanium powder, nickel powder and a binder onto the surface of an iron-base alloy and then heating the iron-base alloy at a temperature of 900.degree.-1200.degree. C. under vacuum so as to form on the surface thereof a layer of the titanium-nickel alloy containing 5-45% by weight of nickel.
摘要翻译: 在其表面的至少一部分上涂覆有含有5-45重量%镍的钛 - 镍合金层的耐腐蚀铁基材料。 该耐腐蚀铁基材料通过将含有钛粉末,镍粉末和粘合剂的粘性涂布液涂覆在铁基合金的表面上,然后在900〜1200℃的温度下加热铁基合金而制造 在真空下在其表面上形成含有5-45重量%镍的钛 - 镍合金层。
-
公开(公告)号:USD653006S1
公开(公告)日:2012-01-24
申请号:US29399169
申请日:2011-08-10
申请人: Kyoji Takahashi
设计人: Kyoji Takahashi
-
公开(公告)号:USD537593S1
公开(公告)日:2007-02-27
申请号:US29252702
申请日:2006-01-26
-
-
-
-