公开(公告)号:US4871604A
公开(公告)日:1989-10-03
申请号:US177221
申请日:1988-04-04
申请人: Lewis R. Hackler
发明人: Lewis R. Hackler
IPC分类号: A47G27/02 , D06M15/00 , D06M23/00 , D06M23/08 , D06M101/00 , D06M101/02 , D06M101/06 , D06M101/08 , D06M101/10 , D06M101/12 , D06M101/16 , D06M101/18 , D06M101/20 , D06M101/22 , D06M101/30 , D06M101/32 , D06M101/34 , D06Q1/14
CPC分类号: D06M23/08 , D06Q1/14 , Y10T428/23921 , Y10T428/23979 , Y10T428/23986 , Y10T428/23993 , Y10T428/2924 , Y10T428/2927
摘要: Pile carpet of nylon, polyester, or other pile yarn, is coated with 0.1 to 5 weight percent, based on weight of the pile yarn of a heat-activated adhesive powder having a melting point within the range of 100.degree. to 170.degree. C., preferably 110.degree. to 150.degree. C. For nylon pile yarn a preferred adhesive powder is a ternary copolyamide selected from the group consisting of 6/6,6/12; 6/6,6/11; and 6/6,6/12,12. The powder is heat-activated, for example to 195.degree. C. for about 60 seconds. The treated carpet displays enhanced carpet tuft appearance, improved resilience, carpet surface cleanness, and improved wear performance.
摘要翻译: 尼龙,聚酯或其他绒毛纱线的地毯,以熔点在100-170℃范围内的热活化粘合剂粉末的绒头纱线的重量为基准涂覆0.1至5重量%。 优选为110℃〜150℃。对于尼龙绒头纱,优选的粘合剂粉末是选自6 / 6,6 / 12的三元共聚酰胺; 6 / 6,6 / 11; 和6 / 6,6 / 12,12。 该粉末被热活化,例如在195℃下热活化约60秒。 经处理的地毯显示增强的地毯毛簇外观,改善的弹性,地毯表面清洁度和改进的磨损性能。
-
公开(公告)号:US4197606A
公开(公告)日:1980-04-15
申请号:US949710
申请日:1978-10-10
CPC分类号: D02J13/00
摘要: The method of this invention comprises the improvement of using an open frame skein carrier with arms to loosely hang the yarn skeins. This allows a shorter total heat-setting time; eliminates kinks, and improves bulk and bulk uniformity of the yarn.
摘要翻译: 本发明的方法包括改进使用具有臂的开放式框架绞纱架以松散地悬挂纱线束。 这允许更短的总热定型时间; 消除扭结,并改善纱线的体积和体积均匀性。
-
公开(公告)号:US5141780A
公开(公告)日:1992-08-25
申请号:US636860
申请日:1991-01-02
IPC分类号: D02G1/12
CPC分类号: D02G1/127
摘要: The invention is directed to a process for producing bulked synthetic multifilament yarn comprising a plurality of continuous synthetic filaments having deposited thereon at intermittent intervals an adhesive polymer component having a melting temperature below that of the continuous synthetic filaments. The process comprises texturizing synthetic multifilament yarn to obtain desired bulk characteristics by directing heated yarn in a current of heated fluid against a yarn plug contained in a texturizing chamber, applying said adhesive polymer component in a molten condition to the surface of said yarn plug, and continuously discharging texturized yarn from said texturizing chamber at a lower linear rate than the feed rate of said yarn to said texturizing zone while said adhesive polymer component is still in a molten but solidifying state, resulting in bulked synthetic multifilament yarn having the adhesive polymer component deposited thereon at intermittent intervals.
摘要翻译: 本发明涉及一种生产膨松的合成复丝纱线的方法,该方法包括多个连续合成细丝,其间隔间隔沉积有熔融温度低于连续合成长丝的粘合剂聚合物组分。 该方法包括通过将加热流体中的加热纱线引导到包含在组织化室中的纱线丝上的加热纱线,将熔融状态下的所述粘合剂聚合物组分施加到所述纱线丝束的表面,从而获得所需的松散特性, 在所述粘合剂聚合物组分仍处于熔融但固化状态的同时,以比所述纱线进给所述织构化区域的进料速率低的线性速率将组织化纱线连续排出,得到具有粘合聚合物组分的膨松合成复丝纱线 间歇地间隔。
-
-