公开(公告)号:US20110305993A1
公开(公告)日:2011-12-15
申请号:US13133701
申请日:2009-12-09
申请人: Li Li , Sokol Ndoni , Rolf Henrik Berg , Lars Schulte , Martin E. Vigild
发明人: Li Li , Sokol Ndoni , Rolf Henrik Berg , Lars Schulte , Martin E. Vigild
CPC分类号: C08J9/0071 , C08J9/26 , C08J9/36 , C08J2201/046 , C08J2300/00 , C08J2353/00
摘要: The present application discloses a method for preparing and rendering hydrophilic a nanoporous material of a polymer matrix which has a porosity of 0.1-90% (v/v), such that the ratio between the fmal water absorption (% (w/w)) and the porosity (% (v/v)) is at least 0.05, the method comprising the steps of: (a) preparing a precursor material comprising at least one polymeric component and having a first phase and a second phase; (b) removal of at least a part of the first phase of the precursor material prepared in step (a) so as to leave behind a nanoporous material of the polymer matrix; (c) irradiating at least a part of said nanoporous material with light of a wave length of in the range of 250-400 nm (or 200-700 nm) in the presence of oxygen and/or ozone. Corresponding hydrophilic nanoporous materials are also disclosed.
摘要翻译: 本申请公开了一种制备和使亲水性的聚合物基质的纳米多孔材料的孔隙率为0.1-90%(v / v)的亲水性方法,使得吸水率(%(w / w)) 并且孔隙率(%(v / v))至少为0.05,该方法包括以下步骤:(a)制备包含至少一种聚合物组分并具有第一相和第二相的前体材料; (b)除去在步骤(a)中制备的前体材料的至少一部分第一相,以留下聚合物基体的纳米多孔材料; (c)在存在氧和/或臭氧的情况下用波长为250-400nm(或200-700nm)的波长照射所述纳米多孔材料的至少一部分。 还公开了相应的亲水纳米多孔材料。
-
公开(公告)号:US08785111B2
公开(公告)日:2014-07-22
申请号:US13133701
申请日:2009-12-09
申请人: Li Li , Sokol Ndoni , Rolf Henrik Berg , Lars Schulte , Martin E. Vigild
发明人: Li Li , Sokol Ndoni , Rolf Henrik Berg , Lars Schulte , Martin E. Vigild
IPC分类号: G03F7/26
CPC分类号: C08J9/0071 , C08J9/26 , C08J9/36 , C08J2201/046 , C08J2300/00 , C08J2353/00
摘要: The present application discloses a method for preparing and rendering hydrophilic a nanoporous material of a polymer matrix which has a porosity of 0.1-90% (v/v), such that the ratio between the final water absorption (% (w/w)) and the porosity (% (v/v)) is at least 0.05, the method comprising the steps of: (a) preparing a precursor material comprising at least one polymeric component and having a first phase and a second phase; (b) removal of at least a part of the first phase of the precursor material prepared in step (a) so as to leave behind a nanoporous material of the polymer matrix; (c) irradiating at least a part of said nanoporous material with light of a wave length of in the range of 250-400 nm (or 200-700 nm) in the presence of oxygen and/or ozone. Corresponding hydrophilic nanoporous materials are also disclosed.