Method for producing nickel-hydrogen cell
    1.
    发明授权
    Method for producing nickel-hydrogen cell 失效
    生产镍氢电池的方法

    公开(公告)号:US06458486B1

    公开(公告)日:2002-10-01

    申请号:US09624638

    申请日:2000-07-25

    IPC分类号: H01M458

    摘要: Since it is possible to optionally adjust the used region of a negative electrode, it is possible to obtain a cell having an excellent balance of durability and discharge characteristic, and it is possible to reduce the resistance of a positive electrode. If only the positive electrode is charged before assembling the cell, it is possible to optionally adjust the used region of the negative electrode, so that it is possible to obtain the cell having the excellent balance of durability and discharge characteristic. Also after a large number of charge and discharge cycles are repeated, it is possible to suppress the internal pressure rise of the cell at the last stage of charge. In addition, it is possible to form a good cobalt conductive network on the active material of the positive electrode, and it is possible to reduce the resistance of the positive electrode.

    摘要翻译: 由于可以可选地调整负极的使用区域,因此可以获得具有优异的耐久性和放电特性的平衡的电池,并且可以降低正极的电阻。 如果在组装电池之前仅使正极充电,则可以可选地调整负极的使用区域,从而可以获得耐久性和放电特性优异的电池。 此外,在重复大量充放电循环之后,可以抑制最后充电阶段的电池的内部压力上升。 另外,可以在正极活性物质上形成良好的钴导电性网络,能够降低正极的电阻。