公开(公告)号:US20060165921A1
公开(公告)日:2006-07-27
申请号:US10563693
申请日:2004-07-02
申请人: Gerard Friour , Oliver Poncelet
发明人: Gerard Friour , Oliver Poncelet
IPC分类号: B41M5/40
CPC分类号: B41M5/5218 , B41M5/5236 , B41M5/5254 , C01B33/26
摘要: The present invention relates to an inkjet recording element having very good dye keeping properties in time. Said inkjet recording element comprises a support and at least one ink-receiving layer, said ink-receiving layer comprising at least one hydrosoluble binder and at least one aluminosilicate polymer obtainable by a preparation method consisting in treating an aluminum halide with a mixture of at least one silicon alkoxide only having hydrolyzable substituents and at least one silicon alkoxide having a non-hydrolyzable substituent, with an aqueous alkali in the presence of silanol groups, the aluminum concentration being maintained less than 0.3 mol/l, the Al/Si molar ratio being maintained between 1 and 3.6 and the alkali/Al molar ratio being maintained between 2.3 and 3; and then stirring the resulting mixture at ambient temperature in the presence of silanol groups for long enough to form the hybrid aluminosilicate polymer. The ink-receiving layer also comprises inorganic particles.
摘要翻译: 本发明涉及在时间上具有非常好的染料保持性的喷墨记录元件。 所述喷墨记录元件包括支撑体和至少一个油墨接收层,所述油墨接收层包含至少一种水溶性粘合剂和至少一种铝硅酸盐聚合物,所述铝硅酸盐聚合物可通过制备方法获得,所述制备方法包括用至少 一个仅具有可水解取代基的硅烷醇盐和至少一种具有不可水解取代基的硅烷氧化物,在硅烷醇基团存在下与碱水溶液接触,铝浓度保持在0.3mol / l以下,Al / Si摩尔比为 保持在1和3.6之间,碱/ Al摩尔比保持在2.3和3之间; 然后在室温下在硅烷醇基团存在下搅拌所得混合物足够长时间以形成混合硅铝酸盐聚合物。 油墨接收层还包含无机颗粒。