公开(公告)号:US20050103158A1
公开(公告)日:2005-05-19
申请号:US10490962
申请日:2002-09-20
Applicant: Pascal Mahot , Guy Nicolas , Marc Voltz
Inventor: Pascal Mahot , Guy Nicolas , Marc Voltz
CPC classification number: C22C1/045 , B22F2998/10 , B22F2999/00 , C22C27/04 , F42B12/74 , B22F1/0003 , B22F1/0088 , B22F3/02 , B22F3/1035 , B22F2201/013
Abstract: Tungsten-based alloy material sintered at a high sintering power that may contain additive elements soluble in the nickel and selected from the group constituted, for example, by rhenium, molybdenum, tantalum, niobium, vanadium or a mixture of these, wherein, after sintering in liquid phase at a temperature of around 1500° C., it has: a two-phased α-γ microstructure that is fully densified, has no porosities or has negligible porosities of a low mean grain size (Lα) and a contiguity (Cαα) that is very low with respect to the size of the tungsten crystals, and a dispersion of micro-oxides with no loss of ductility properties.
Abstract translation: 以高烧结能烧结的钨基合金材料,其可以含有可溶于镍的添加元素,并且选自例如由铼,钼,钽,铌,钒或它们的混合物组成的组,其中烧结后 在液相中在约1500℃的温度下,它具有:完全致密化的两相α-γ微观结构,没有孔隙度或具有低平均晶粒尺寸(Lalpha)和邻接性(Calphaalpha)的孔隙度可忽略 ),其相对于钨晶体的尺寸非常低,并且微量氧化物的分散体没有延展性的损失。
-
公开(公告)号:US07226492B2
公开(公告)日:2007-06-05
申请号:US10490962
申请日:2002-09-20
Applicant: Pascal Mahot , Guy Nicolas , Marc Voltz
Inventor: Pascal Mahot , Guy Nicolas , Marc Voltz
CPC classification number: C22C1/045 , B22F2998/10 , B22F2999/00 , C22C27/04 , F42B12/74 , B22F1/0003 , B22F1/0088 , B22F3/02 , B22F3/1035 , B22F2201/013
Abstract: Tungsten-based alloy material sintered at a high sintering power that may contain additive elements soluble in the nickel and selected from the group constituted, for example, by rhenium, molybdenum, tantalum, niobium, vanadium or a mixture of these, wherein, after sintering in liquid phase at a temperature of around 1500° C., it has: a two-phased α-γ microstructure that is fully densified, has no porosities or has negligible porosities of a low mean grain size (Lα) and a contiguity (Cαα) that is very low with respect to the size of the tungsten crystals, and a dispersion of micro-oxides with no loss of ductility properties.
Abstract translation: 以高烧结能烧结的钨基合金材料,其可以含有可溶于镍的添加元素,并且选自例如由铼,钼,钽,铌,钒或它们的混合物组成的组,其中烧结后 在液相中在约1500℃的温度下,它具有:完全致密化的两相α-γ微观结构,没有孔隙率或具有低平均晶粒尺寸(Lalpha)和邻接性(Calphaalpha)的孔隙度可忽略 ),其相对于钨晶体的尺寸非常低,并且微量氧化物的分散体没有延展性的损失。
-