摘要: A method for producing carbon paper, including: 1) employing a polyacrylonitrile-based carbon fiber as a reinforcing material, a phenolic resin or epoxy resin as a bonding agent, and molding and preparing the carbon fiber into a carbon fiber blank by a dry paper-making method; and 2) stacking and putting a product obtained in step 1) into a reaction furnace for deposition process, the pressure in the reaction furnace being 1 kPa to 1 atmosphere, with methane, propene, or liquefied petroleum gas as a carbon source gas, nitrogen or argon gas as a diluent gas, the concentration of the carbon source gas being 5-100%, the gas flow rate being 0.1-5 L/min, and the temperature in the reaction furnace being controlled at between 800° C. and 1100° C., and the time of deposition process being 1-5 h.
摘要翻译: 一种生产碳纸的方法,包括:1)使用聚丙烯腈类碳纤维作为增强材料,酚醛树脂或环氧树脂作为粘合剂,并通过干纸将碳纤维成型和制备成碳纤维坯料 制作方法; 和2)将步骤1)中得到的产品堆放并放入用于沉积工艺的反应炉中,反应炉中的压力为1kPa至1大气压,其中甲烷,丙烯或液化石油气为碳源气体,氮气 或氩气作为稀释气体,碳源气体的浓度为5〜100%,气体流量为0.1〜5L / min,反应炉内的温度控制在800℃〜1100℃ ℃,沉积时间为1-5小时。
-
公开(公告)号:US08652567B2
公开(公告)日:2014-02-18
申请号:US13474796
申请日:2012-05-18
申请人: Zhiyong Xie , Qizhong Huang , Zhean Su , Mingyu Zhang , Jianxun Chen , Boyun Huang
发明人: Zhiyong Xie , Qizhong Huang , Zhean Su , Mingyu Zhang , Jianxun Chen , Boyun Huang
IPC分类号: B05D3/02
CPC分类号: D21H13/50 , C04B35/83 , C04B2235/425 , C04B2235/48 , C04B2235/614 , C04B2235/616 , C04B2235/77
摘要: A method for producing carbon paper, including: 1) employing a polyacrylonitrile-based carbon fiber as a reinforcing material, a phenolic resin or epoxy resin as a bonding agent, and molding and preparing the carbon fiber into a carbon fiber blank by a dry paper-making method; and 2) stacking and putting a product obtained in step 1) into a reaction furnace for deposition process, the pressure in the reaction furnace being 1 kPa to 1 atmosphere, with methane, propene, or liquefied petroleum gas as a carbon source gas, nitrogen or argon gas as a diluent gas, the concentration of the carbon source gas being 5-100%, the gas flow rate being 0.1-5 L/min, and the temperature in the reaction furnace being controlled at between 800° C. and 1100° C., and the time of deposition process being 1-5 h.
摘要翻译: 一种生产碳纸的方法,包括:1)使用聚丙烯腈类碳纤维作为增强材料,酚醛树脂或环氧树脂作为粘合剂,并通过干纸将碳纤维成型和制备成碳纤维坯料 制作方法; 和2)将步骤1)中得到的产品堆放并放入用于沉积工艺的反应炉中,反应炉中的压力为1kPa至1大气压,其中甲烷,丙烯或液化石油气为碳源气体,氮气 或氩气作为稀释气体,碳源气体的浓度为5〜100%,气体流量为0.1〜5L / min,反应炉内的温度控制在800℃〜1100℃ ℃,沉积时间为1-5小时。
-