公开(公告)号:US20100219178A1
公开(公告)日:2010-09-02
申请号:US12396254
申请日:2009-03-02
Applicant: Mike M. Ghiran , Susan E. Hartfield-Wunsch , John E. Carsley
Inventor: Mike M. Ghiran , Susan E. Hartfield-Wunsch , John E. Carsley
IPC: B23K13/01
CPC classification number: B23K13/01
Abstract: The present invention provides a method and device for inductively heating a first and second surface to form a closure assembly. A method contemplated by the present invention includes spacing an upper die from a lower die for receipt of the first surface and the second surface configured in an overlying orientation, securing one end of the first surface to an end of the second surface and compressing the first surface toward the second surface to form a compressed arrangement which is inductively heated into a closure assembly.
Abstract translation: 本发明提供了一种用于感应加热第一和第二表面以形成封闭组件的方法和装置。 本发明考虑的方法包括将上模与下模间隔开以接收第一表面,而第二表面以上覆方向构造,将第一表面的一端固定到第二表面的端部并压缩第一表面 表面朝向第二表面以形成被感应加热到封闭组件中的压缩布置。
-
公开(公告)号:US08592733B2
公开(公告)日:2013-11-26
申请号:US12396254
申请日:2009-03-02
Applicant: Mike M. Ghiran , Susan E. Hartfield-Wunsch , John E. Carsley
Inventor: Mike M. Ghiran , Susan E. Hartfield-Wunsch , John E. Carsley
IPC: B23K13/01
CPC classification number: B23K13/01
Abstract: The present invention provides a method and device for inductively heating a first and second surface to form a closure assembly. A method contemplated by the present invention includes spacing an upper die from a lower die for receipt of the first surface and the second surface configured in an overlying orientation, securing one end of the first surface to an end of the second surface and compressing the first surface toward the second surface to form a compressed arrangement which is inductively heated into a closure assembly.
Abstract translation: 本发明提供了一种用于感应加热第一和第二表面以形成封闭组件的方法和装置。 本发明考虑的方法包括将上模与下模间隔开以接收第一表面,而第二表面以上覆方向构造,将第一表面的一端固定到第二表面的端部并压缩第一表面 表面朝向第二表面以形成被感应加热到封闭组件中的压缩布置。
-
公开(公告)号:US08211251B2
公开(公告)日:2012-07-03
申请号:US12541441
申请日:2009-08-14
Applicant: John E. Carsley , Chih-Cheng Hsu , Susan E. Hartfield-Wunsch , Theresa M Lee , James G. Schroth
Inventor: John E. Carsley , Chih-Cheng Hsu , Susan E. Hartfield-Wunsch , Theresa M Lee , James G. Schroth
IPC: C22F1/04
CPC classification number: C22F1/047 , C21D2221/00 , C22C21/08
Abstract: A method of accomplishing precipitation hardening of a selected portion of an aluminum panel is disclosed herein. The method includes identifying at least one area of the aluminum panel that experiences thermal stress above a threshold value during a bake cycle, thereby identifying the selected portion. Prior to the bake cycle, the method further includes locally heating the selected portion at a predetermined temperature for a predetermined time sufficient to increase a local yield strength of the selected portion such that the increased local yield strength ranges from 150 MPa to 300 MPa.
Abstract translation: 本文公开了一种实现铝板的选定部分的沉淀硬化的方法。 该方法包括在烘烤循环期间识别经历热应力高于阈值的铝面板的至少一个区域,从而识别所选择的部分。 在烘烤循环之前,该方法还包括在预定温度下将所选择的部分局部加热预定时间,足以提高所选部分的局部屈服强度,使得增加的局部屈服强度范围为150MPa至300MPa。
-
公开(公告)号:US20110036472A1
公开(公告)日:2011-02-17
申请号:US12541441
申请日:2009-08-14
Applicant: John E. Carsley , Chih-Cheng Hsu , Susan E. Hartfield-Wunsch , Theresa M. Lee , James G. Schroth
Inventor: John E. Carsley , Chih-Cheng Hsu , Susan E. Hartfield-Wunsch , Theresa M. Lee , James G. Schroth
CPC classification number: C22F1/047 , C21D2221/00 , C22C21/08
Abstract: A method of accomplishing precipitation hardening of a selected portion of an aluminum panel is disclosed herein. The method includes identifying at least one area of the aluminum panel that experiences thermal stress above a threshold value during a bake cycle, thereby identifying the selected portion. Prior to the bake cycle, the method further includes locally heating the selected portion at a predetermined temperature for a predetermined time sufficient to increase a local yield strength of the selected portion such that the increased local yield strength ranges from 150 MPa to 300 MPa.
Abstract translation: 本文公开了一种实现铝板的选定部分的沉淀硬化的方法。 该方法包括在烘烤循环期间识别经历热应力高于阈值的铝面板的至少一个区域,从而识别所选择的部分。 在烘烤循环之前,该方法还包括在预定温度下将所选择的部分局部加热预定时间,足以提高所选部分的局部屈服强度,使得增加的局部屈服强度范围为150MPa至300MPa。
-
-
-