Aluminum brazin sheet
    1.
    发明申请
    Aluminum brazin sheet 有权
    铝布片

    公开(公告)号:US20060134451A1

    公开(公告)日:2006-06-22

    申请号:US10543150

    申请日:2003-09-26

    IPC分类号: B32B15/01

    摘要: An aluminum brazing sheet has a core material made of an aluminum alloy and a cladding material cladded on at least one side of the core material and made of an aluminum alloy having a potential lower than that of the core material. The cladding material is made of an aluminum alloy consisting essentially of 0.4 to 0.7 mass % of Mg, 0.5 to 1.5 mass % of Si, and 0.4 to 1.2 mass % of Mn, the remainder being Al and unavoidable impurities. Zn in the amount of 6 mass % or less is added in accordance with need. An aluminum brazing sheet having not only high strength but also less pressure adhesion failure and excellent productivity can be obtained.

    摘要翻译: 铝钎焊片具有由铝合金制成的芯材和包覆在芯材的至少一侧上的包层材料,并且由铝合金制成,其电位低于芯材的电位。 包层材料由铝合金制成,其基本上由Mg组成为0.4〜0.7质量%,Si为0.5〜1.5质量%,Mn为0.4〜1.2质量%,余量为Al和不可避免的杂质。 根据需要加入6质量%以下的Zn。 可以获得不仅具有高强度,而且还具有较低压力粘附破坏和优异的生产率的铝钎焊板。

    Aluminum brazing sheet
    2.
    发明授权
    Aluminum brazing sheet 有权
    铝钎焊板

    公开(公告)号:US08283049B2

    公开(公告)日:2012-10-09

    申请号:US10543150

    申请日:2003-09-26

    IPC分类号: B32B15/20 C22C21/00

    摘要: An aluminum brazing sheet has a core material made of an aluminum alloy and a cladding material cladded on at least one side of the core material and made of an aluminum alloy having a potential lower than that of the core material. The cladding material is made of an aluminum alloy consisting essentially of 0.4 to 0.7 mass % of Mg, 0.5 to 1.5 mass % of Si, and 0.4 to 1.2 mass % of Mn, the remainder being Al and unavoidable impurities. Zn in the amount of 6 mass % or less is added in accordance with need. An aluminum brazing sheet having not only high strength but also less pressure adhesion failure and excellent productivity can be obtained.