Isocyanate-curing coating material and method for application thereof
    1.
    发明授权
    Isocyanate-curing coating material and method for application thereof 失效
    异氰酸酯固化涂料及其应用方法

    公开(公告)号:US5981660A

    公开(公告)日:1999-11-09

    申请号:US895263

    申请日:1997-07-16

    摘要: An isocyanate-curing coating material is disclosed which essentially consists of (A) an agent formed of a hydroxyl group-containing polymer having a weight average molecular weight in the range of 1000-20000 and (B) a polyisocyanate compound as a curing agent containing at least three isocyanate groups in the molecular unit thereof and having a weight average molecular weight in the range of 400-3000 and incorporating (A) the agent and (B) the curing agent in such amounts that the isocyanate groups in (B) the curing agent amounts to 0.5-2 equivalent weights per equivalent weight of the hydroxyl group in (A) the agent. A method for spray coating the isocyanate-curing coating material is also disclosed which comprises the steps of mixing (A) the agent with (B) the curing agent in a coating device, heating the resultant mixture therein to a temperature in the range of 35-80.degree. C., and spraying the hot mixture directly on a given object with the coating device.

    摘要翻译: 公开了一种异氰酸酯固化涂料,其基本上由(A)由重均分子量在1000-20000的含羟基的聚合物形成的试剂和(B)作为固化剂的多异氰酸酯化合物 其分子单元中至少有三个异氰酸酯基团,其重均分子量在400-3000范围内,并且(A)试剂和(B)固化剂的含量使得(B)中的异氰酸酯基团 固化剂相当于(A)试剂中每当量羟基的0.5-2当量。 还公开了喷雾涂覆异氰酸酯固化涂料的方法,该方法包括以下步骤:将涂料与(B)固化剂混合在一起,将其中的所得混合物加热至35℃ -80℃,并用涂覆装置将热混合物直接喷涂在给定的物体上。