Method for treatment of chemically passivated galvanized surfaces to improve paint adhesion
    1.
    发明申请
    Method for treatment of chemically passivated galvanized surfaces to improve paint adhesion 有权
    用于处理化学钝化镀锌表面以改善涂料附着力的方法

    公开(公告)号:US20060289089A1

    公开(公告)日:2006-12-28

    申请号:US11453963

    申请日:2006-06-14

    申请人: Thomas Cape

    发明人: Thomas Cape

    IPC分类号: C23C22/34

    摘要: A method of treating a zinc-galvanized metal surface, which has been chemically passivated, the treatment providing increased resistance to corrosion and improved adherence to a subsequently applied organic coating comprising contacting a chromium passivated, zinc-galvanized metal surface with a coating solution bath comprising from about 1 to about 10 parts per thousand, based on fluorine content, of an inorganic acid or ion that contains fluorine; at least 0.5 parts per thousand, based on transition metal cation content, of an oxide and/or a salt of nickel; and optionally, from about 0 to about 3.0 grams per liter of a polymer selected from the group consisting of polyacrylic acid, polymethacrylic acid, and C1 to C8 alkanol esters thereof; wherein the pH of the solution is from about 2.0 to 3.6 and the temperature of the solution is at least 60° C.; and thereafter sealing the treated surface.

    摘要翻译: 一种处理已被化学钝化的镀锌金属表面的方法,该处理提供增加的耐腐蚀性和改善对随后施加的有机涂层的粘附性,包括使铬钝化的镀锌金属表面与包含溶液浴接触,所述涂覆溶液浴包含 基于含氟量的约1至约10份的含氟的无机酸或离子; 基于过渡金属阳离子含量,至少0.5份/分的氧化物和/或镍盐; 和任选的约0至约3.0克/升的选自聚丙烯酸,聚甲基丙烯酸和C 1至C 8烷基链烷醇酯的聚合物 ; 其中溶液的pH为约2.0至3.6,溶液的温度为至少60℃; 然后密封经处理的表面。