Optical glass, preform for precision press molding and method of manufacturing thereof, optical element and method of manufacturing thereof
    1.
    发明授权
    Optical glass, preform for precision press molding and method of manufacturing thereof, optical element and method of manufacturing thereof 有权
    光学玻璃,精密加压成型用预成型体及其制造方法,光学元件及其制造方法

    公开(公告)号:US07745361B2

    公开(公告)日:2010-06-29

    申请号:US11723468

    申请日:2007-03-20

    CPC分类号: C03C3/068

    摘要: The present invention relates to an optical glass having a refractive index (nd) of greater than or equal to 1.65 and an Abbé number (ν (nu)d) of greater than or equal to 50 for use in precision press molding. The glass exhibits that a ratio α (alpha)1/α (alpha)2 is less than 17 when temperature denoting maximum value of differential in amount of elongation of glass relative to temperature differential DELTAT (where DELTAT denotes a constant value of 1° C. or less) over a temperature range from glass transition temperature (Tg) to sag temperature (Ts) is denoted as T1, average coefficient of linear expansion over a range from T1−5° C. to T1+5° C. is denoted as alpha1, and average coefficient of linear expansion over a range from the glass transition temperature (Tg)−160° C. to the glass transition temperature (Tg)−140° C. is denoted as alpha2.

    摘要翻译: 本发明涉及一种折射率(nd)大于或等于1.65的光学玻璃和用于精密压模成型的大于或等于50的Abbé数(ngr(nu)d)。 玻璃表明当温度表示相对于温差DELTAT的玻璃的伸长量的微分值的最大值时,α(α)1 /α(α)2的比值小于17(其中,ΔTt表示1℃的常数值 表示为从玻璃化转变温度(Tg)至下垂温度(Ts)的温度范围为T1,表示在T1-5℃〜T1 + 5℃的范围内的平均线膨胀系数 作为α1,在玻璃化转变温度(Tg)-160℃至玻璃化转变温度(Tg)-140℃的范围内的平均线膨胀系数表示为α2。

    Optical glass, precision press molding preform and optical element
    2.
    发明授权
    Optical glass, precision press molding preform and optical element 失效
    光学玻璃,精密压模成型预制件和光学元件

    公开(公告)号:US07670978B2

    公开(公告)日:2010-03-02

    申请号:US11494506

    申请日:2006-07-28

    IPC分类号: C03C3/066 C03C3/068

    摘要: The optical glass has a refractive index of equal to or greater than 1.65 and an Abbé number ranging from 50 to 60. In the optical glass, as molar basis, a ratio of SiO2 content to B2O3 content is greater than 0.5 and equal to or less than 0.90; a total content of SiO2 and B2O3 ranges from 50 to 70 percent; Li2O content ranges from 5 to 20 percent; La2O3 content ranges from 0.5 to 22 percent; a ratio of ZnO content to RO (MgO, CaO, SrO and BaO) is equal to or greater than 0.5; a total content of Gd2O3, Y2O3 and Yb2O3 ranges from 1 to 15 percent; Sb2O3 content ranges from 0 to 1 percent; and no BaO is comprised, or a ratio of the total content of La2O3, Gd2O3, Y2O3 and Yb2O3 to the content of BaO is equal to or greater than 10.

    摘要翻译: 光学玻璃具有等于或大于1.65的折射率,范围为50至60的Abbé数。在光学玻璃中,以摩尔计为基准,SiO 2含量与B 2 O 3含量的比率大于0.5并且等于或小于 大于0.90; SiO2和B2O3的总含量范围为50-70%; Li2O含量在5%至20%之间; La2O3含量范围为0.5〜22%; ZnO含量与RO(MgO,CaO,SrO和BaO)的比例等于或大于0.5; Gd 2 O 3,Y 2 O 3和Yb 2 O 3的总含量为1〜15%。 Sb2O3含量范围为0〜1% 并且不包含BaO,或者La2O3,Gd2O3,Y2O3和Yb2O3的总含量与BaO的含量的比例等于或大于10。

    Optical glass, precision press-molding preform, process for producing the preform, optical element and process for producing the element
    3.
    发明申请
    Optical glass, precision press-molding preform, process for producing the preform, optical element and process for producing the element 有权
    光学玻璃,精密压制成型预型件,用于制造预成型件的工艺,光学元件以及用于制造元件的方法

    公开(公告)号:US20090288450A1

    公开(公告)日:2009-11-26

    申请号:US12457821

    申请日:2009-06-23

    IPC分类号: C03B23/00

    CPC分类号: C03C3/068 C03B11/08

    摘要: An optical glass having high refractivity and a low sag temperature and having a low-temperature softening property that enables precision press-molding is provided, and the optical glass contains, by mol %, 5 to 50% of B2O3, 3 to 50% of SiO2, 5 to 40% of TiO2, 1 to 40% of ZnO, 5 to 20% of La2O3, 0 to 10% of Gd2O3, 0 to 15% of Nb2O5, 0 to 10% of ZrO2, 0 to 5% of Ta2O5, 0 to 10% of Bi2O3, 0 to 10% of MgO, 0 to 8% of CaO, 0 to 10% of SrO, 0 to 10% of BaO, provided that the total content of MgO, CaO, SrO and BaO is 15% or less, 0 to 20% of Li2O, and 0 to 5% of Na2O, optionally containing Sb2O3 as a refining agent, and having a refractive index (nd) of 1.8 or more and an Abbe's number (vd) of 35 or less.

    摘要翻译: 提供具有高折射率和低下垂温度并具有能够进行精密加压成型的低温软化性的光学玻璃,光学玻璃含有5〜50%的B 2 O 3,3〜50%的 SiO2,5〜40%的TiO2,1〜40%的ZnO,5〜20%的La2O3,0〜10%的Gd2O3,0〜15%的Nb2O5,0〜10%的ZrO2,0〜5%的Ta2O5 ,0〜10%的Bi2O3,0〜10%的MgO,0〜8%的CaO,0〜10%的SrO,0〜10%的BaO,条件是MgO,CaO,SrO和BaO的总含量为 15%以下,0〜20%的Li 2 O,0〜5%的Na 2 O,任选含有Sb 2 O 3作为澄清剂,折射率(nd)为1.8以上,阿贝数(vd)为35或 减。

    Optical glass, precision press-molding preform, process for production thereof, optical element and process for the production thereof
    4.
    发明授权
    Optical glass, precision press-molding preform, process for production thereof, optical element and process for the production thereof 有权
    光学玻璃,精密压制成型预成型件,其制造方法,光学元件及其制造方法

    公开(公告)号:US07351675B2

    公开(公告)日:2008-04-01

    申请号:US11038495

    申请日:2005-01-21

    IPC分类号: C03C3/068 C03C3/095

    摘要: An optical glass taking account of meltability and the moldability of a preform, having optical constants including a refractive index (nd) of at least 1.57 but less than 1.67 and an Abbe's number (νd) of over 55 but not more than 65, having the property of softening at a low temperature and being suitable as a glass for precision press-molding, the optical glass including an optical glass containing B2O3, SiO2, La2O3, Gd2O3, an alkali metal oxide and an alkaline earth metal oxide as essential components, having a B2O3 and SiO2 total content of 52% by weight or more and having an SiO2/B2O3 content ratio of from 0.38 to 1.2, and an optical glass wherein the relationship of the refractive index (nd) and the Abbe's number (νd) satisfies the equation (1), νd>260−126×nd.   (1)

    摘要翻译: 考虑到熔融性和预型件的成型性的光学玻璃,其具有包括折射率(nd)至少为1.57但小于1.67的光学常数和超过55但不大于65的阿贝数(nud),其具有 在低温下软化的性质并且适合作为精密加压成型的玻璃,所述光学玻璃包括含有B 2 O 3 3,SiO 2的光学玻璃, 2 2,2 3,3 3,N 2 O 3,碱金属氧化物和 碱土金属氧化物作为必要组分,具有52重量%以上的B 2 N 3 O 3和SiO 2 2总含量,并具有 SiO 2含量比为0.38〜1.2的光学玻璃,其中折射率(nd)/ 并且阿贝数(nud)满足等式(1),<?in-line-formula description =“In-line Formulas”end =“lead”?> nud> 260-126xnd。 (1)<?in-line-formula description =“In-line Formulas”end =“tail”?>

    Optical glass, precision press molding preform and manufacturing method of the same, optical element and manufacturing method of the same
    5.
    发明申请
    Optical glass, precision press molding preform and manufacturing method of the same, optical element and manufacturing method of the same 失效
    光学玻璃,精密压模成型预制件及其制造方法相同,光学元件及其制造方法相同

    公开(公告)号:US20070032366A1

    公开(公告)日:2007-02-08

    申请号:US11494506

    申请日:2006-07-28

    摘要: The optical glass has a refractive index of equal to or greater than 1.65 and an Abbé number ranging from 50 to 60. In the optical glass, as molar basis, a ratio of SiO2 content to B2O3 content is greater than 0.5 and equal to or less than 0.90; a total content of SiO2 and B2O3 ranges from 50 to 70 percent; Li2O content ranges from 5 to 20 percent; La2O3 content ranges from 0.5 to 22 percent; a ratio of ZnO content to RO (MgO, CaO, SrO and BaO) is equal to or greater than 0.5; a total content of Gd2O3, Y2O3 and Yb2O3 ranges from 1 to 15 percent; Sb2O3 content ranges from 0 to 1 percent; and no BaO is comprised, or a ratio of the total content of La2O3, Gd2O3, Y2O3 and Yb2O3 to the content of BaO is equal to or greater than 10.

    摘要翻译: 光学玻璃具有等于或大于1.65的折射率和从50至60的Abbé数。在光学玻璃中,以摩尔计,SiO 2含量与B 2 <3 O 3含量大于0.5且等于或小于0.90; SiO 2和B 2 O 3 3的总含量在50-70%的范围内; Li 2 O 2含量范围为5%至20%; La 2 O 3 3含量范围为0.5%至22%; ZnO含量与RO(MgO,CaO,SrO和BaO)的比例等于或大于0.5; Gd 2 N 3 O 3,Y 2 O 3和Y b 2的总含量 O 3范围为1至15%; Sb 2 O 3 3含量为0至1%; 并且不包含BaO,或者La 2 O 3 O 3的总含量,Gd 2 O 3 3 / >,Y 2 O 3 3和Y b 2 O 3 3相对于BaO的含量等于或大于 10。

    Optical glass, press-molding preform and optical element
    6.
    发明授权
    Optical glass, press-molding preform and optical element 有权
    光学玻璃,预成型件和光学元件

    公开(公告)号:US07087543B2

    公开(公告)日:2006-08-08

    申请号:US10608435

    申请日:2003-06-30

    CPC分类号: C03C3/095 Y10S501/903

    摘要: An optical glass having a refractive index (nd) of 1.57 to 1.67, an Abbe's number (νd) of 55 to 65 and a glass transition temperature (Tg) of 560° C. or lower and having a low-temperature softening property and excellent climate resistance or a haze value of 3% or less, or an optical glass comprising, by mol %, 22 to 40% of B2O3, 12 to 40% of SiO2, 2 to 20% of Li2O, 5 to 15% of CaO, 2 to 14% of ZnO, 0.5 to 4% of La2O3, 0 to 3% of Gd2O3, 0 to 3% of Y2O3, the total content of La2O3, Gd2O3 and Y2O3 being at least 1%, 0 to 5% of Al2O3, 0 to 3% of ZrO2 and 0 to 5% of BaO, the total content of the above components being more than 96%, and having a refractive index (nd) of 1.57 to 1.67 and an Abbe's number (νd) of 55 to 65.

    摘要翻译: 折射率(nd)为1.57〜1.67,阿贝数(nud)为55〜65,玻璃化转变温度(Tg)为560℃以下且具有低温软化性和优异的光学玻璃 耐气候性或雾度值为3%以下,或者含有摩尔%22〜40%的B 2 O 3 3的光学玻璃,12〜40% 的SiO 2,2〜20%的Li 2 O,5〜15%的CaO,2〜14%的ZnO,0.5〜4%的La 2 O 3, 2%O 3,0〜3%的Gd 2 O 3 3,0〜3%的Y 2 < 3 O 3,3 O 3,3 O 3,3 N 3 O 3的总含量 和/或Y 2 O 3 3以及至少1%,0至5%的Al 2 O 3 3 / 0〜3%的ZrO 2和0〜5%的BaO,上述成分的总含量大于96%,折射率(nd)为1.57〜1.67 阿贝数(nud)为55至65。

    Optical glass, precision press-molding preform, process for producing the preform, optical element and process for producing the element
    7.
    发明申请
    Optical glass, precision press-molding preform, process for producing the preform, optical element and process for producing the element 审中-公开
    光学玻璃,精密压制成型预型件,用于制造预成型件的工艺,光学元件以及用于制造元件的方法

    公开(公告)号:US20060105900A1

    公开(公告)日:2006-05-18

    申请号:US11273621

    申请日:2005-11-15

    IPC分类号: C03C3/095 C03C3/068

    CPC分类号: C03C3/068 C03B11/08

    摘要: An optical glass having high refractivity and a low sag temperature and having a low-temperature softening property that enables precision press-molding is provided, and the optical glass contains, by mol %, 5 to 50% of B2O3, 3 to 50% of SiO2, 5 to 40% of TiO2, 1 to 40% of ZnO, 5 to 20% of La2O3, 0 to 10% of Gd2O3, 0 to 15% of Nb2O5, 0 to 10% of ZrO2, 0 to 5% of Ta2O5, 0 to 10% of Bi2O3, 0 to 10% of MgO, 0 to 8% of CaO, 0 to 10% of SrO, 0 to 10% of BaO, provided that the total content of MgO, CaO, SrO and BaO is 15% or less, 0 to 20% of Li2O, and 0 to 5% of Na2O, optionally containing Sb2O3 as a refining agent, and having a refractive index (nd) of 1.8 or more and an Abbe's number (vd) of 35 or less.

    摘要翻译: 提供了具有高折射率和低下垂温度并具有能够进行精密加压成型的低温软化性能的光学玻璃,并且光学玻璃含有摩尔%为5〜50%的B 2, 3〜50%的SiO 2,5〜40%的TiO 2,1〜40%的ZnO,5 至20%的O 2 O 3,0至10%的Gd 2 O 3 3,0至15 Nb 2 O 5的%,ZrO 2的0〜10%,Ta 2 O 5的0〜5% O 5,0〜10%的Bi 2 O 3 3,0〜10%的MgO,0〜8%的CaO,0〜 10%的SrO,0〜10%的BaO,条件是MgO,CaO,SrO和BaO的总含量为15%以下,0〜20%的Li 2 O,0〜 5%的Na 2 O,任选地含有Sb 2 O 3 3 3,作为澄清剂,并且折射率(nd)为1.8或 阿贝数(vd)为35以下。

    Optical glass, preform for precision press-molding, process for the production of the preform, optical element, and process for the production of the element

    公开(公告)号:US20060079390A1

    公开(公告)日:2006-04-13

    申请号:US11225886

    申请日:2005-09-14

    IPC分类号: C03C3/095 C03C3/068 C03C3/066

    CPC分类号: C03C3/068

    摘要: An optical glass which has an Abbe's number (νd) of 50 to 59, has the property of not easily reacting with a press mold, a low-temperature softening property, excellent glass stability and high refractivity, and is suitable for precision press-molding. The optical glass comprising B2O3 and SiO2 as essential components and having a B2O3 and SiO2 total content (B2O3+SiO2) of 45 to 70 by mol % and an SiO2 content/B2O3 content molar ratio (SiO2/B2O3) of from 0.1 to 0.5, the optical glass further comprising, by mol %, 5 to 15% of La2O3, 0.1 to 8% of Gd2O3, provided that the total content of La2O3 and Gd2O3 is 8% or more, 0 to 10% of Y2O3, 3 to 18% of Li2O, provided that the molar ratio of the content of Li2O to the total content of B2O3 and SiO2 [Li2O/(B2O3+SiO2)] is over 0 but not more than 0.2, 0.1 to 15% of ZnO, 2 to 20% of CaO, 0 to 5% of BaO, provided that the content of BaO is smaller than the content of ZnO, 0 to 5% of SrO, 0 to 5% of MgO, provided that the molar ratio of the total content of MgO, CaO, SrO and BaO to the total content of B2O3 and SiO2 [(MgO+CaO+SrO+BaO)/(B2O3+SiO2) is from 0.1 to 0.4, and 0 to 5% of ZrO2, and having a refractive index (nd) and an Abbe's number (νd) which satisfy the equation (1), νd≧308.5−150×nd (in which 50≦νd≦59)   (1)

    Optical glass, precision press-molding preform, process for production thereof, optical element and process for the production thereof
    9.
    发明申请
    Optical glass, precision press-molding preform, process for production thereof, optical element and process for the production thereof 有权
    光学玻璃,精密压制成型预成型件,其制造方法,光学元件及其制造方法

    公开(公告)号:US20050164864A1

    公开(公告)日:2005-07-28

    申请号:US11038495

    申请日:2005-01-21

    摘要: An optical glass taking account of meltability and the moldability of a preform, having optical constants including a refractive index (nd) of at least 1.57 but less than 1.67 and an Abbe's number (νd) of over 55 but not more than 65, having the property of softening at a low temperature and being suitable as a glass for precision press-molding, the optical glass including an optical glass containing B2O3, SiO2, La2O3, Gd2O3, an alkali metal oxide and an alkaline earth metal oxide as essential components, having a B2O3 and SiO2 total content of 52% by weight or more and having an SiO2/B2O3 content ratio of from 0.38 to 1.2, and an optical glass wherein the relationship of the refractive index (nd) and the Abbe's number (νd) satisfies the equation (1), νd>260−126×nd  (1).

    摘要翻译: 考虑到熔融性和预型件的成型性的光学玻璃,其具有包括折射率(nd)至少为1.57但小于1.67的光学常数和超过55但不大于65的阿贝数(nud),其具有 在低温下软化的性质并且适合作为精密加压成型的玻璃,所述光学玻璃包括含有B 2 O 3 3,SiO 2的光学玻璃, 2 2,2 3,3 3,N 2 O 3,碱金属氧化物和 碱土金属氧化物作为必要组分,具有52重量%以上的B 2 N 3 O 3和SiO 2 2总含量,并具有 SiO 2含量比为0.38〜1.2的光学玻璃,其中折射率(nd)/ 并且阿贝数(nud)满足等式(1),<?in-line-formula description =“In-line Formulas”end =“lead”?> nud> 260-126xnd(1)。<?in-line -fo rmulae description =“在线公式”end =“tail”?>

    PREFORMS FOR PRECISION PRESS MOLDING, OPTICAL ELEMENTS, AND METHODS OF MANUFACTURING THE SAME
    10.
    发明申请
    PREFORMS FOR PRECISION PRESS MOLDING, OPTICAL ELEMENTS, AND METHODS OF MANUFACTURING THE SAME 审中-公开
    精密压模成型,光学元件及其制造方法

    公开(公告)号:US20110289970A1

    公开(公告)日:2011-12-01

    申请号:US13171082

    申请日:2011-06-28

    CPC分类号: C03C3/21 C03C3/062 C03C3/16

    摘要: Preforms for precision press molding made of optical glass, optical elements, and methods of manufacturing the same are provided. The preforms are suited to precision press molding having a broad range of dispersion characteristics, a low glass transition temperature, a low sag point, and good resistance to devitrification while containing no PbO. The optical element is obtained by precision press molding the preform. One example of the preform has a refractive index (nd) of greater than or equal to 1.7 and an Abbé number (νd) of less than or equal to 32. The other example of the preform has an Abbé number (νd) exceeding 32.

    摘要翻译: 提供了由光学玻璃,光学元件及其制造方法制成的精密压制成型的预制件。 预成型件适合于具有宽范围的分散特性,低玻璃化转变温度,低凹陷点以及良好的耐失透性同时不含PbO的精密压模成型。 光学元件通过精密压模成型而获得。 预型件的一个示例具有大于或等于1.7的折射率(nd)和小于或等于32的Abbé数(&ngr; d)。预成型件的另一个实例具有Abbé数(&ngr; d )超过32。