公开(公告)号:US5847050A
公开(公告)日:1998-12-08
申请号:US793449
申请日:1997-03-03
IPC分类号: C08C1/065 , C08C1/14 , C08F279/02 , C08F285/00 , C08L25/06 , C08L27/06 , C08L51/04
CPC分类号: C08L51/04 , C08C1/065 , C08C1/14 , C08F279/02 , C08F285/00 , C08L25/06 , C08L27/06
摘要: A method for particles agglomeration and enlargement of a diene type polymer rubber latex, which comprises subjecting a diene type polymer rubber latex produced by emulsion polymerization, to particles agglomeration and enlargement to obtain a particles-enlarged diene type polymer rubber latex (A), wherein the particles enlargement is allowed to take place by agglomeration based mainly on Brownian coagulation; a graft copolymer (B) of a particles-enlarged diene type polymer rubber latex (A) obtained by the above method; and a thermoplastic resin composition comprising said graft copolymer (B).
摘要翻译: PCT No.PCT / JP96 / 01854 Sec。 371日期1997年3月3日 102(e)1997年3月3日PCT PCT 1997年7月4日PCT公布。 出版物WO97 / 02295 日期1997年1月23日一种二聚型聚合物橡胶胶乳的颗粒聚集和扩大的方法,其包括将通过乳液聚合制备的二烯类聚合物橡胶胶乳进行颗粒附聚和扩大以获得增大二甲基聚合物橡胶胶乳 (A),其中通过主要基于布朗凝固的聚集使颗粒增大发生; 通过上述方法获得的增大二聚型聚合物橡胶胶乳(A)的接枝共聚物(B); 和包含所述接枝共聚物(B)的热塑性树脂组合物。
-
公开(公告)号:US06407167B1
公开(公告)日:2002-06-18
申请号:US09743786
申请日:2001-03-12
申请人: Koichi Shishido , Akira Nakata
发明人: Koichi Shishido , Akira Nakata
IPC分类号: C08L6700
CPC分类号: C08L67/02 , C08F279/02 , C08L51/04 , C08L67/025 , C08L69/00 , C08F220/10 , C08L2666/14 , C08L2666/02
摘要: A resin composition comprises (A) a polycarbonate resin, (B) a saturated polyester resin and/or polyester-based elastomer, and (C) a copolymer obtained by graft-polymerizing a given monomer in the presence of latex containing a butadiene-based rubber polymer. The graft copolymer is obtained under the following conditions (a) to (c): (a) the polymerization formulation is composed of 60 to 90% by weight of the butadiene-based rubber polymer and 10 to 40% by weight of the monomer, (b) the monomer formulation of the latex is composed of 50 to 100% by weight of butadiene and 0 to 50% by weight of vinyl-based monomers copolymerized with butadiene, and (c) the latex has a weight-average particle size from 100 to 200 nm, and the ratio dw/dn of the weight-average particle size to the number-average particle size is 1 or more and 3 or less. According to the present invention, a thermoplastic resin composition excellent in production stability and having excellent impact resistance and molded appearance is provided.
摘要翻译: 树脂组合物包含(A)聚碳酸酯树脂,(B)饱和聚酯树脂和/或聚酯类弹性体,和(C)通过在含有丁二烯类的胶乳存在下将给定的单体接枝聚合而得到的共聚物 橡胶聚合物。 在以下条件(a)〜(c)中得到接枝共聚物:(a)聚合配方由丁二烯系橡胶系聚合物的60〜90重量%,单体的10〜40重量% (b)胶乳的单体配方由丁二烯50至100重量%和与丁二烯共聚的乙烯基系单体0至50重量%组成,(c)胶乳的重均粒径为 100〜200nm,重均粒径与数均粒径的比dw / dn为1以上3以下。 根据本发明,提供了生产稳定性优异且耐冲击性优异且成型外观优异的热塑性树脂组合物。
-