摘要: A process for manufacturing a high tensile steel wire, characterized by comprising the steps of pre-cooling a hot-rolled steel rod to a temperature between 750.degree.-900.degree. C. by means of a cooling apparatus provided between a group of intermediate rolling mills and a group of finishing rolling mills in a hot rolling line for steel rod, finishing rolling the thus pre-cooled steel rod, quenching the hot rolled steel rod to a temperature of 700.degree. C. or lower to provide a supercooled austenite phase, then finishing-cooling the thus quenched rod to provide martensite, and drawing the resulting steel rod with roller dies without descaling is disclosed.
摘要翻译: 一种制造高强度钢丝的方法,其特征在于包括以下步骤:通过设置在一组中间轧机之间的冷却装置将热轧钢棒预冷至750-900℃的温度 和一组用于钢棒的热轧生产线的精轧机,对这样预冷的钢棒进行精轧,将热轧钢棒淬火至700℃以下,提供过冷奥氏体相, 对如此淬火的棒进行精加工冷却以提供马氏体,并且公开了将所得钢棒用辊模而不进行除锈。