公开(公告)号:US09309434B2
公开(公告)日:2016-04-12
申请号:US13878435
申请日:2011-10-19
申请人: Ali Rihan , Anthony J. Tye
发明人: Ali Rihan , Anthony J. Tye
IPC分类号: C09D133/14 , C09D133/08 , C08G18/36 , C08G18/62 , C08G18/65 , C09D175/04
CPC分类号: C09D133/14 , C08G18/36 , C08G18/6229 , C08G18/6254 , C08G18/6547 , C09D175/04 , Y10T428/31551
摘要: Scratch resistance and/or reflow of a refinish topcoat is improved by preparing the topcoat from a refinish topcoat coating composition comprising an unsaturated fatty acid ester polyol that does not undergo oxidative cure when the applied refinish topcoat coating composition is cured.
摘要翻译: 通过从包含不饱和脂肪酸酯多元醇的修补面漆涂料组合物制备面漆可以改善涂层顶涂层的耐擦伤性和/或回流性能,所述不饱和脂肪酸酯多元醇在施用的修补面漆涂料组合物固化时不进行氧化固化。
-
公开(公告)号:US20130202893A1
公开(公告)日:2013-08-08
申请号:US13878435
申请日:2011-10-19
申请人: Ali Rihan , Anthony J. Tye
发明人: Ali Rihan , Anthony J. Tye
IPC分类号: C09D133/14
CPC分类号: C09D133/14 , C08G18/36 , C08G18/6229 , C08G18/6254 , C08G18/6547 , C09D175/04 , Y10T428/31551
摘要: Scratch resistance and/or reflow of a refinish topcoat is improved by preparing the topcoat from a refinish topcoat coating composition comprising an unsaturated fatty acid ester polyol that does not undergo oxidative cure when the applied refinish topcoat coating composition is cured.
摘要翻译: 通过从包含不饱和脂肪酸酯多元醇的修补面漆涂料组合物制备面漆可以改善涂层顶涂层的耐擦伤性和/或回流性能,所述不饱和脂肪酸酯多元醇在施用的修补面漆涂料组合物固化时不进行氧化固化。
-
公开(公告)号:US07446149B2
公开(公告)日:2008-11-04
申请号:US09965423
申请日:2001-09-27
申请人: Ali Rihan , Emerson Keith Colyer
发明人: Ali Rihan , Emerson Keith Colyer
CPC分类号: B05D7/534 , C08G18/6229 , C08L2205/02 , C09D133/066 , C09D175/04 , C08L2666/04
摘要: A refinish clearcoat composition includes an hydroxyl-functional acrylic polymer. The acrylic polymer has a number average molecular weight of at least about 5000 and is polymerized using at least about 45% by weight cycloaliphatic monomer, based on total monomer weight polymerized. The clearcoat composition is fast drying. Optionally, the clearcoat is cured by low temperature baking. The cured clearcoat surface may be taped without leaving tape marks as soon as the substrate is cooled. The cured clearcoat may undergo wet sanding after baking as soon as the part is cooled, and can then be buffed back to a high gloss finish after sanding and washing.
摘要翻译: 修补透明涂料组合物包括羟基官能的丙烯酸聚合物。 基于聚合的单体总重量,丙烯酸类聚合物的数均分子量为至少约5000,并且使用至少约45重量%的脂环族单体进行聚合。 透明涂料组合物快速干燥。 任选地,透明涂层通过低温烘烤固化。 只要衬底被冷却,固化的透明涂层表面可以被胶带而不留痕迹。 固化的透明涂层可以在烘烤后立即进行湿式砂磨,一旦冷却,然后在磨砂和洗涤后可以抛光回高光泽度。
-
-