Abstract:
To supply a consumer (13a, 13b) with liquid carbon dioxide with a desired temperature of more than 0° C. and a desired pressure of more than 30 bar, liquid carbon dioxide is taken from a tank (1) in which it is stored at a temperature below the desired temperature and a pressure below the desired pressure. The pressure of the carbon dioxide is increased (3) and subsequently the carbon dioxide is heated to the desired temperature (14a, 14b).
Abstract:
In a method of producing a casting, molding or pressing tool (1) or tool insert (2) with at least one material layer (3, 5, 7) and with temperature control medium channels (6) arranged in the at least one material layer (3, 5, 7), the temperature control medium channels (6) are introduced into the at least one material layer (3, 5, 7) using a thermal spray process (2).
Abstract:
For supplying a sink with liquid carbon dioxide with a required temperature of more than 0° C. and with a required pressure of more than 30 bar, liquid carbon dioxide is taken from a tank, in which it has been stored at a temperature below the required temperature and at a pressure below the required pressure. The pressure of the carbon dioxide is increased and then the carbon dioxide is heated to the required temperature.
Abstract:
A process and device is provided for cooling extruded hollow sections, especially pipes, that are made of plastic. Liquid or supercritical carbon dioxide is directed into the interior of the plastic hollow section through an extruder head and is depressurized in at least one depressurization nozzle, whereby carbon dioxide in gaseous and solid form is produced. The carbon dioxide that is in gaseous form is directed to the inner wall of the hollow section, while carbon dioxide snow is brought into heat exchange with the inner wall of hollow section only to the extent that the latter is not damaged.
Abstract:
A method for producing a molded part, wherein a molten polymer is introduced into a mold space of a molding tool and liquid carbon dioxide with a pressure of at least 160 bar, preferably with a pressure of at least 200 bar or at least 250 bar is supplied to the mold space, whereby the polymer is pressed against the walls of the mold space and a space is formed in the polymer.
Abstract:
A method for producing plastic parts by a gas injection molding method by injecting a melt into a cavity and a flushing gas is fed into the cavity prior to the injection of the melt.