GLASS COMPOSITION, GLASS SUBSTRATE FOR FLAT PANEL DISPLAY USING THE SAME, FLAT PANEL DISPLAY, AND METHOD FOR PRODUCING GLASS SUBSTRATE FOR FLAT PANEL DISPLAY
    1.
    发明申请
    GLASS COMPOSITION, GLASS SUBSTRATE FOR FLAT PANEL DISPLAY USING THE SAME, FLAT PANEL DISPLAY, AND METHOD FOR PRODUCING GLASS SUBSTRATE FOR FLAT PANEL DISPLAY 审中-公开
    玻璃组合物,用于使用其的平板显示器的玻璃基板,平板显示器和用于生产用于平板显示器的玻璃基板的方法

    公开(公告)号:US20130345041A1

    公开(公告)日:2013-12-26

    申请号:US14015495

    申请日:2013-08-30

    CPC classification number: C03C3/091

    Abstract: Provided is a glass composition suitable for a glass substrate for a flat panel display such as a liquid crystal display. This glass composition has high thermal stability, and is substantially free of BaO but has a low devitrification temperature. It is suitable for the production of a glass substrate by a downdraw process. This glass composition contains, in terms of mass %: 54 to 62% of SiO2; 4 to 11% of B2O3; 15 to 20% of Al2O3; 2 to 5% of MgO; 0 to 7% of CaO; 0 to 13.5% of SrO; 0 to 1% of K2O; 0 to 1% of SnO2; and 0 to 0.2% of Fe2O3, and is substantially free of BaO. In this glass composition, the total content of alkaline earth metal oxides (MgO+CaO+SrO) is 10 to 18.5 mass %. The devitrification temperature of the glass composition is 1200° C. or lower.

    Abstract translation: 提供一种适用于液晶显示器等平板显示器的玻璃基板的玻璃组合物。 该玻璃组合物具有高的热稳定性,并且基本上不含BaO但具有低失透温度。 适用于通过下拉工艺生产玻璃基板。 该玻璃组合物以质量%计含有54〜62%的SiO 2, 4〜11%的B2O3; 15〜20%的Al2O3; 2〜5%的MgO; 0〜7%的CaO; 0〜13.5%的SrO; 0〜1%K2O; 0〜1%的SnO2; 和0〜0.2%的Fe 2 O 3,并且基本上不含BaO。 在该玻璃组合物中,碱土类金属氧化物(MgO + CaO + SrO)的总含量为10〜18.5质量%。 玻璃组合物的失透温度为1200℃以下。