Abstract:
The invention concerns a method for producing pulverulent hardening accelerators by reactive spray drying, where an aqueous phase I comprising calcium ions, and an aqueous phase II comprising sulphate ions, the molar ratio of the calcium ions to the sulphate ions being from 1/5 to 5/1, are contacted at a spray nozzle, and the phases I and II contacted with one another at the spray nozzle are sprayed in a streaming environment of drying gas. Likewise concerned are the pulverulent hardening accelerators producible by the method of the invention, and their use for accelerating the hardening of bassanite and/or anhydrite with formation of gypsum.