公开(公告)号:US10676604B2
公开(公告)日:2020-06-09
申请号:US15767330
申请日:2016-10-21
Applicant: BOREALIS AG
Inventor: Norbert Reichelt , Paul De Mink , Markus Gahleitner , Katja Klimke , Dietrich Gloger
IPC: C08L23/12 , C08F299/00
Abstract: The invention relates to long-chain branched polypropylene composition (b-PPC) comprising at least one long-chain branched propylene homopolymer or copolymer (b-PP) and at least one linear propylene homopolymer or copolymer (l-PP). The long-chain branched polypropylene composition (b-PPC) being suitable for foam application.
-
公开(公告)号:US20180298174A1
公开(公告)日:2018-10-18
申请号:US15767330
申请日:2016-10-21
Applicant: BOREALIS AG
Inventor: Norbert Reichelt , Paul De Mink , Markus Gahleitner , Katja Klimke , Dietrich Gloger
IPC: C08L23/12
Abstract: The invention relates to long-chain branched polypropylene composition (b-PPC) comprising at least one long-chain branched propylene homopolymer or copolymer (b-PP) and at least one linear propylene homopolymer or copolymer (1-PP). The long-chain branched polypropylene composition (b-PPC) being suitable for foam application.
-
公开(公告)号:US20200087478A1
公开(公告)日:2020-03-19
申请号:US16467202
申请日:2017-12-28
Applicant: Borealis AG
Inventor: Hermann Braun , Norbert Reichelt , Andreas Fuchs , Alexander Standler , Paul De Mink , Markus Gahleitner
Abstract: The invention relates to a process for the production of a foam having low organic compounds emissions, to polypropylene foamed products obtainable by the process, and to a process for the manufacture of low organic compounds emission articles comprising a foam for use in cars and food packaging. The process comprises the steps of: a) providing a foam comprising a propylene composition comprising a high melt strength propylene (HMS-PP) homopolymer or copolymer or combinations thereof, said HMS-PP foam having a melt strength of at least 25 cN at a maximum speed of at least 200 mm/s and a melting temperature of at least 135° C. and b) subjecting the HMS-PP foam to a thermal treatment at a temperature Tt which is preferably between 5 and 15° C. below the melting temperature Tm of the HMS-PP for a duration between preferably 1 and 10 minutes.
-
-