PRECIPITATION HARDENING STEEL WITH IMPROVED TOUGHNESS AND METHOD
    1.
    发明申请
    PRECIPITATION HARDENING STEEL WITH IMPROVED TOUGHNESS AND METHOD 审中-公开
    具有改进的韧性和方法的降低硬化钢

    公开(公告)号:US20160138122A1

    公开(公告)日:2016-05-19

    申请号:US14038229

    申请日:2013-09-26

    Inventor: Colin Fletcher

    Abstract: In some aspects, a heat treatment process is described for precipitation hardening steel. The heat treatment process can include a solution treatment for a precipitation hardening steel part. The solution treatment includes heating the precipitation hardening steel part to an austenitizing temperature. The heat treatment process can also include a quenching or cooling treatment, in which the precipitation hardening steel part is cooled to a martensitizing temperature. The heat treatment process can also include an aging treatment, in which the precipitation hardening steel part is heated to a temperature of 1000° F. and held at that temperature for five or more hours until a fracture toughness of the precipitation hardening steel part is greater than 120 ksi√in.

    Abstract translation: 在一些方面,描述了用于沉淀硬化钢的热处理工艺。 热处理工艺可以包括沉淀硬化钢部件的固溶处理。 固溶处理包括将沉淀硬化钢部分加热至奥氏体化温度。 热处理工艺还可以包括淬火或冷却处理,其中沉淀硬化钢部分被冷却至马氏平
    坦化温度。 热处理工序也可以包括时效处理,其中将析出硬化钢部分加热到1000°F的温度,并在该温度下保持5小时以上,直到析出硬化钢部分的断裂韧性更大 超过120ksi√in。