Abstract:
Blow molded article comprising a propylene copolymer having a MFR2 (230° C.) in the range of more than 2.0 to 12.0 g/10 min, a comonomer content in the range of 4.0 to below 4.0 mol.-%, a melting temperature in the range of 125 to below 143° C., and a xylene cold soluble fraction (XCS) in the range of above 15.0 to 40.0 wt.-%.
Abstract:
Blow molded article comprising a propylene copolymer having a MFR2 (230° C.) in the range of more than 2.0 to 12.0 g/10 min, a comonomer content in the range of 4.0 to below 4.0 mol.-%, a melting temperature in the range of 125 to below 143° C., and a xylene cold soluble fraction (XCS) in the range of above 15.0 to 40.0 wt.-%.