1.
公开(公告)号:US20220017700A2
公开(公告)日:2022-01-20
申请号:US16768342
申请日:2018-11-30
Applicant: COMMSCOPE CONNECTIVITY BELGIUM BVBA
Inventor: Valja EVERAERT , Kristel VAN RENTERGHEM , Lydia AERTGEETS , Ana NEDELCHEVA HRISTOVA
Abstract: Disclosed herein are methods of preparing thermoplastic gels and dry silicone gels with an alkyl ester polydimethylsiloxane having a formula (I): (I) Also disclosed are thermoplastic gels and dry silicone gels prepared by the disclosed methods. In the formula (I), n is about 60% to about 90% of the formula (I); m is about 10% to about 40% of the formula (I); R is —(C═O)—OR1; and R is a C2-C20 alkyl group. The alkyl ester polydimethylsiloxane has a weight average molecular weight of about 10,000 g/mol to about 50,000 g/mol. The hardness of the thermoplastic gels is less than 120 g peak load. The hardness of the dry silicone gels is less than 100 g peak load.
-
2.
公开(公告)号:US20210171717A1
公开(公告)日:2021-06-10
申请号:US16768342
申请日:2018-11-30
Applicant: COMMSCOPE CONNECTIVITY BELGIUM BVBA
Inventor: Valja EVERAERT , Kristel VAN RENTERGHEM , Lydia AERTGEETS , Ana NEDELCHEVA HRISTOVA
Abstract: Disclosed herein are methods of preparing thermoplastic gels and dry silicone gels with an alkyl ester polydimethylsiloxane having a formula (I): (I) Also disclosed are thermoplastic gels and dry silicone gels prepared by the disclosed methods. In the formula (I), n is about 60% to about 90% of the formula (I); m is about 10% to about 40% of the formula (I); R is —(C═O)—OR1; and R is a C2-C20 alkyl group. The alkyl ester polydimethylsiloxane has a weight average molecular weight of about 10,000 g/mol to about 50,000 g/mol. The hardness of the thermoplastic gels is less than 120 g peak load. The hardness of the dry silicone gels is less than 100 g peak load.
-