FAST FIRING METHOD FOR HIGH POROSITY CERAMICS
    3.
    发明申请
    FAST FIRING METHOD FOR HIGH POROSITY CERAMICS 有权
    高度陶瓷的快速燃烧方法

    公开(公告)号:US20150028528A1

    公开(公告)日:2015-01-29

    申请号:US13951840

    申请日:2013-07-26

    IPC分类号: B29D24/00

    摘要: A method for firing a green honeycomb ceramic body including heating the green honeycomb ceramic body from room temperature to a first temperature of less than or equal to about 350° C. with at least one heating rate of greater than or equal to about 80° C./hr. The green honeycomb ceramic body may be heated from the first temperature to a second temperature of greater than or equal to about 800° C. at a heating rate of greater than or equal to about 90° C./hr. The green honeycomb ceramic body may be heated from the second temperature to a third temperature of greater than or equal to about 1000° C. The green honeycomb ceramic body may include aluminum raw materials for forming an aluminum titanate ceramic body.

    摘要翻译: 一种焙烧生坯蜂窝陶瓷体的方法,包括将生坯蜂窝陶瓷体从室温加热至小于或等于约350℃的第一温度,至少一个加热速率大于或等于约80℃ ./hr。 绿色蜂窝陶瓷体可以以大于或等于约90℃/ hr的加热速率从第一温度加热至大约或等于约800℃的第二温度。 绿色蜂窝陶瓷体可以从第二温度加热到大于或等于约1000℃的第三温度。生坯蜂窝陶瓷体可以包括用于形成钛酸铝陶瓷体的铝原料。