摘要:
There is provided a thermoplastic elastomer composition, comprising per 100 parts by weight of ethylene-propylene-diene monomer (EPDM), 20 to 30 parts by weight of polypropylene (PP), 7 to 30 parts by weight of ethylene octene rubber (EOR), 7 to 23 parts by weight of propylene butene rubber (PBR), and 55 to 65 parts by weight of mineral oil, wherein a content of said poly(1-butene) (PB) is small parts by weight. Thereby, there can be provided a thermoplastic elastomer composition and a molded member obtained by molding the same, which can be superior in the shape recovery property at the deformation, without deteriorating the tactile quality, gloss-change resistance, or formability of particles.
摘要:
The thermoplastic elastomer composition of this invention includes 2 through 14 mass % of PP; 19 through 35 mass % of PB-1; and 30 through 52 mass % of olefin-based rubber, and a weight ratio of PB-1/(PP+PB-1) is 56 through 90% and a weight ratio of PB-1/(PP+(PB-1)+olefin-based rubber) is 25 through 47%.
摘要:
A thermoplastic elastomer composition for an operating member, comprising high-crystalline polypropylene having crystallinity of 95% or more, low-crystalline polypropylene having crystallinity of less than 95%, poly(1-butene), partial-cross-linked olefin family rubber having SP value of 7.5 or more and 8.5 or less, and non-cross-linked olefin family rubber having SP value of 7.5 or more and 8.5 or less. Accordingly, there can be provided the thermoplastic elastomer composition for an operating member and the molded member obtained by molding the same, which can provide the better tactic quality and improve the wear resistance and scratch resistance.
摘要:
A polypropylene-based resin composition suitable for molding of especially an automobile bumper having good formability, high rigidity, excellent appearance, and high surface impact strength is provided. This composition includes: 30-62 wt. % of a propylene copolymer having an MFR of 40-70 g/10 min.; 5-20 wt. % of a propylene-based block copolymer including a crystalline polypropylene part having a high MFR and a specific ethylene-propylene copolymer part and having an MFR of 100-130 g/10 min; 10-20 wt. % of two types of ethylene-α-olefin copolymer elastomers each having a specific MFR and a specific density; and 23-30 wt. % of talc having a specific particle size.