1.
公开(公告)号:US07968030B2
公开(公告)日:2011-06-28
申请号:US11909950
申请日:2006-03-27
Applicant: Christopher W Newton , Steven R Allen , Steven D Moore
Inventor: Christopher W Newton , Steven R Allen , Steven D Moore
CPC classification number: D01F6/74
Abstract: The present invention relates to processes for hydrolyzing polyphosphoric acid in spun multifilament yarns.
Abstract translation: 本发明涉及在纺丝复丝纱中水解多磷酸的方法。
-
2.
公开(公告)号:US07906615B2
公开(公告)日:2011-03-15
申请号:US11909659
申请日:2006-03-27
Applicant: Steven R Allen , Steven D Moore , Christopher W Newton , David J Rodini , Doetze Jakob Sikkema
Inventor: Steven R Allen , Steven D Moore , Christopher W Newton , David J Rodini , Doetze Jakob Sikkema
CPC classification number: D01D10/06 , D01F6/74 , Y10T428/2913
Abstract: The present invention relates to processes for hydrolyzing polyphosphoric acid in a fiber and the removal of hydrolyzed polyphosphoric acid from the fiber.
Abstract translation: 本发明涉及水解纤维中的多磷酸和从纤维中除去水解的多磷酸的方法。
-
公开(公告)号:US07776246B2
公开(公告)日:2010-08-17
申请号:US11909934
申请日:2006-03-27
Applicant: Steven R Allen , Steven D Moore , Christopher William Newton , David J Rodini , Doetze Jakob Sikkema
Inventor: Steven R Allen , Steven D Moore , Christopher William Newton , David J Rodini , Doetze Jakob Sikkema
IPC: B29C47/88
CPC classification number: D01F6/74
Abstract: The present invention concerns a process for making a polyareneazole multifilament yarn comprising: a) extruding a solution comprising polyareneazole polymer and polyphosphoric acid through a plurality of orifices to produce filaments; b) forming a multifilament yarn from said filaments; c) hydrolyzing at least some of the polyphosphoric acid in the yarn by heating the yarn to a temperature above about 120° C. for up to about two minutes; d) washing at least some of the hydrolyzed polyphosphoric acid from the yarn; e) drying the washed yarn; f) optionally, heating the yarn above about 300° C., and g) collecting the yarn at a speed of at least about 50 meters per minute.
Abstract translation: 本发明涉及一种制备聚芳腈复丝纱线的方法,包括:a)通过多个孔口挤出包含聚芳腈聚合物和多磷酸的溶液以产生长丝; b)从所述长丝形成复丝纱线; c)通过将纱线加热至约120℃以上的温度,使纱线中的至少一些多磷酸水解至多约2分钟; d)从纱线中洗涤至少一些水解的多磷酸; e)干燥洗涤的纱线; f)任选地,将纱线加热到约300℃以上,g)以至少约50米/分钟的速度收集纱线。
-
-