    摘要: A method for producing microfine fibers having low resistance to deformation and high elasticity in accordance with the present invention comprises acts of: (a) providing polymer A and polymer B; (b) melting polymer A and polymer B to make a filament; (c) drawn the filament to make a staple fiber; (d) entangling the staple fiber to form a non-woven; (e) impregnating the non-woven with a impregnating agent; and may further comprise the acts of (f) using polyurethane impregnating the nonwoven with the impregnating agent or without the impregnating agent; (g) coagulating the non-woven with dimethylformamide (DMF); (h) washing the non-woven with hot water; (i) impregnating the non-woven with a treatment agent; (j) abrading the non-woven to attain a split type mirofine fiber substrate; and (k) bonding a coating to the microfine fiber substrate. Therefore, the method can attain an artificial leather product having low resistance to deformation and high elasticity.

    摘要翻译: 根据本发明的生产具有低变形和高弹性的微细纤维的方法包括以下动作:(a)提供聚合物A和聚合物B; (b)熔化聚合物A和聚合物B以制成长丝; (c)拉丝以制成短纤维; (d)缠绕短纤维以形成无纺布; (e)用浸渍剂浸渍无纺布; 并且可以进一步包括(f)使用浸渍所述非织造布的聚氨酯浸渍剂或不含浸渍剂的作用; (g)用二甲基甲酰胺(DMF)凝结无纺布; (h)用热水洗涤无纺布; (i)用处理剂浸渍无纺布; (j)研磨无纺布以获得分裂型微纤维基材; 和(k)将涂层粘结到微细纤维基材上。 因此,该方法可以获得具有低变形性和高弹性的人造革制品。