Abstract:
The present invention provides a process for thermosetting pitch fibers in reduced times, at low concentrations of oxygen and at higher temperatures than previously possible. Additionally, the present invention provides a pitch fiber which has an oxygen diffusion rate to the center of the fiber which is competitive with the rate of oxidation at the fiber's surface. Further, the present invention provides a high density pitch fiber batt which thermosets without loss of fiber structure.
Abstract:
A solvating component for a solvated mesophase pitch. The solvated component includes a mixture of aromatic hydrocarbons having boiling points in the atmospheric equivalent boiling point range of about 285null to about 500null C. (about 550null F.-932null F.). At least 80% of the carbon atoms of the hydrocarbons are aromatic as characterized by carbon 13 NMR. The aromatic hydrocarbons are selected from a group consisting of aromatic compounds having 2 to 5 aromatic rings, substituted aromatic compounds having 2 to 5 aromatic rings wherein said substituents are alkyl groups having 1 to 3 carbons, hydroaromatic compounds having 2 to 5 rings, substituted aromatic compounds having 2 to 5 rings wherein said substituents are alkyl groups having 1 to 3 carbons, and mixtures thereof.