Abstract:
A ceramic precursor batch composition comprising inorganic ceramic-forming ingredients, a hydrophobically modified cellulose ether binder having a molecular weight less than or equal to about 300,000 g/mole and an aqueous solvent is provided. The ceramic precursor batch composition has a ratio of binder to aqueous solvent of less than about 0.32. The ceramic precursor batch composition may be used to increase the rate of extrusion of the composition. A method for increasing a rate of extrusion of a ceramic precursor batch composition is also disclosed.