公开(公告)号:US20100307430A1
公开(公告)日:2010-12-09
申请号:US12303764
申请日:2007-06-07
申请人: Daniel Petelot , Annie Fouquet , Catheline Petelot , Emilie Petelot , Adeline Petelot , Jean Leyer , Bruno Vandenberghe , Viviane Lepingle , Ghislain Louis
发明人: Daniel Petelot , Annie Fouquet , Catheline Petelot , Emilie Petelot , Adeline Petelot , Jean Leyer , Bruno Vandenberghe , Viviane Lepingle , Ghislain Louis
CPC分类号: C22C38/02 , C22C38/04 , C22C38/22 , C22C38/44 , Y10S148/909
摘要: The invention concerns steels having excellent resistance over time, in a corrosive atmosphere due to oxidizing environments such as, for example, fumes or water vapour, under high pressure and/or temperature. The invention concerns a steel composition for special applications, said composition containing, by weight, about 1.8 to 11% of chromium (and preferably between about 2.3 and 10% of chromium), less than 1% of silicon, and between 0.20 and 0.45% of manganese. It has been found that it is possible to adjust the contents of the composition based on a predetermined model, selected to obtain substantially optimal properties with respect to corrosion in specific conditions of high temperature performances. Said model can involve as additive of as residue at least one element selected among molybdenum, tungsten, cobalt, and nickel.
摘要翻译: 本发明涉及在高压和/或高温下由于诸如烟雾或水蒸汽之类的氧化性环境而在腐蚀性气氛中具有优异的耐久性的钢。 本发明涉及一种用于特殊用途的钢组合物,所述组合物含有约1.8-11%的铬(优选约2.3-10%的铬),小于1%的硅和0.20-0.45%的铬, 的锰。 已经发现,可以基于预定模型来调整组合物的含量,该预定模型被选择以获得关于在高温性能的特定条件下的腐蚀的基本上最佳的性能。 所述模型可以包括作为残留物的添加剂,其选自钼,钨,钴和镍中的至少一种元素。
-
公开(公告)号:US09005520B2
公开(公告)日:2015-04-14
申请号:US12303764
申请日:2007-06-07
申请人: Jean Leyer , Bruno Vandenberghe , Viviane Lepingle , Ghislain Louis , Annie Fouquet , Catheline Petelot , Emilie Petelot , Adeline Petelot
CPC分类号: C22C38/02 , C22C38/04 , C22C38/22 , C22C38/44 , Y10S148/909
摘要: The invention concerns steels having excellent resistance over time, in a corrosive atmosphere due to oxidizing environments such as, for example, fumes or water vapor, under high pressure and/or temperature. The invention concerns a steel composition for special applications, said composition containing, by weight, about 1.8 to 11% of chromium (and preferably between about 2.3 and 10% of chromium), less than 1% of silicon, and between 0.20 and 0.45% of manganese. It has been found that it is possible to adjust the contents of the composition based on a predetermined model, selected to obtain substantially optimal properties with respect to corrosion in specific conditions of high temperature performances. Said model can involve as additive of as residue at least one element selected among molybdenum, tungsten, cobalt, and nickel.
摘要翻译: 本发明涉及在高压和/或高温下由于诸如烟雾或水蒸汽之类的氧化性环境而在腐蚀性气氛中具有优异的耐久性的钢。 本发明涉及一种用于特殊用途的钢组合物,所述组合物含有约1.8-11%的铬(优选约2.3-10%的铬),小于1%的硅和0.20-0.45%的铬, 的锰。 已经发现,可以基于预定模型来调整组合物的含量,该预定模型被选择以获得关于在高温性能的特定条件下的腐蚀的基本上最佳的性能。 所述模型可以包括作为残留物的添加剂,其选自钼,钨,钴和镍中的至少一种元素。
-