公开(公告)号:US09873958B2
公开(公告)日:2018-01-23
申请号:US15437245
申请日:2017-02-20
发明人: Randy E. Pepper , Mridula Babli Kapur , Gert J. Claasen , Edward N. Knickerbocker , Nathan J. Wiker , William J. Michie, Jr. , Mark B. Davis
CPC分类号: D01F6/30 , C08F210/02 , C08L23/04 , C08L23/0815 , C08L2205/02 , C08L2205/16 , C08L2314/06 , D01D5/08 , D01D5/10 , D01D5/12 , D01D10/02 , D01F6/04 , D04H1/56 , D04H3/007 , D04H3/16 , Y10T428/249921 , Y10T442/30 , Y10T442/3976 , Y10T442/60 , C08L2666/06
摘要: Fibers made a polyethylene composition, and method of making the same. The polyethylene composition comprises less than or equal to 100 percent by weight of the units derived from ethylene and less than 20 percent by weight of units derived from one or more α-olefin comonomers; wherein said polyethylene composition has a density in the range of 0.930 to 0.960 g/cm3, a molecular weight distribution (Mw/Mn) in the range of 1.70 to 3.5, a melt index (I2) in the range of 1 to 300 g/10 minutes, a molecular weight distribution (Mz/Mw) in the range of less than 2.5, a shear viscosity in the range of 20 to 250 Pascal-s at 3000 s−1 shear rate measured at 190° C., vinyl unsaturation of less than 0.1 vinyls per one thousand carbon atoms present in the backbone of said composition; and wherein the fiber is a monocomponent meltspun fiber.
-
公开(公告)号:US20170159211A1
公开(公告)日:2017-06-08
申请号:US15437245
申请日:2017-02-20
发明人: Randy E. Pepper , Mridula Babli Kapur , Gert J. Claasen , Edward N. Knickerbocker , Nathan J. Wiker , William J. Michie, JR. , Mark B. Davis
CPC分类号: D01F6/30 , C08F210/02 , C08L23/04 , C08L23/0815 , C08L2205/02 , C08L2205/16 , C08L2314/06 , D01D5/08 , D01D5/10 , D01D5/12 , D01D10/02 , D01F6/04 , D04H1/56 , D04H3/007 , D04H3/16 , Y10T428/249921 , Y10T442/30 , Y10T442/3976 , Y10T442/60 , C08L2666/06
摘要: Fibers made a polyethylene composition, and method of making the same. The polyethylene composition comprises less than or equal to 100 percent by weight of the units derived from ethylene and less than 20 percent by weight of units derived from one or more α-olefin comonomers; wherein said polyethylene composition has a density in the range of 0.930 to 0.960 g/cm3, a molecular weight distribution (Mw/Mn) in the range of 1.70 to 3.5, a melt index (I2) in the range of 1 to 300 g/10 minutes, a molecular weight distribution (Mz/Mw) in the range of less than 2.5, a shear viscosity in the range of 20 to 250 Pascal-s at 3000 s−1 shear rate measured at 190° C., vinyl unsaturation of less than 0.1 vinyls per one thousand carbon atoms present in the backbone of said composition; and wherein the fiber is a monocomponent meltspun fiber.
-