公开(公告)号:US20210147589A1
公开(公告)日:2021-05-20
申请号:US17091217
申请日:2020-11-06
Applicant: ExxonMobil Chemical Patents Inc.
Inventor: Porter C. Shannon , Handel D. Bennett , Nathaniel B. Guy , Daniel G. O'Neil , James L. Schulze , Michael G. Tribo
IPC: C08F210/02 , C08J5/18 , C09K3/10
Abstract: Polyethylene copolymers with a structure that provides improved film properties are provided. The copolymers can have a density of about 0.905 to about 0.911 g/cm3. The copolymers can also have a DRI/I2 ratio of about 0.0008 to about 0.060, an I2 value of about 0.6 to about 3.8 dg/min, and an I21 value of about 8 to about 57 dg/min. The copolymers having those properties can be produced by introducing ethylene and at least one other olefin comonomer to a single reactor at a comonomer/ethylene mole ratio of about 0.02 to about 0.03 and polymerizing at a temperature of about 76.7° C. to about 80.6° C. and a pressure of about 1,724 kPa to about 2,413 kPa. The copolymers can be used to make films having a 21 mol % O2 transmission rate of about 150 to about 200 cc/100 in2/24 hr. and hot tack seal initiation temperatures of about 65° C. to 80° C.
-
公开(公告)号:US11767384B2
公开(公告)日:2023-09-26
申请号:US17091217
申请日:2020-11-06
Applicant: ExxonMobil Chemical Patents Inc.
Inventor: Porter C. Shannon , Handel D. Bennett , Nathaniel B. Guy , Daniel G. O'Neil , James L. Schulze , Michael G. Tribo
IPC: C08F210/02 , C08J5/18 , C09K3/10 , C08F210/14
CPC classification number: C08F210/02 , C08F210/14 , C08J5/18 , C09K3/10 , C08F2800/10 , C08J2323/08 , C09K2200/062
Abstract: Polyethylene copolymers with a structure that provides improved film properties are provided. The copolymers can have a density of about 0.905 to about 0.911 g/cm3. The copolymers can also have a DRI/I2 ratio of about 0.0008 to about 0.060, an I2 value of about 0.6 to about 3.8 dg/min, and an I21 value of about 8 to about 57 dg/min. The copolymers having those properties can be produced by introducing ethylene and at least one other olefin comonomer to a single reactor at a comonomer/ethylene mole ratio of about 0.02 to about 0.03 and polymerizing at a temperature of about 76.7° C. to about 80.6° C. and a pressure of about 1,724 kPa to about 2,413 kPa. The copolymers can be used to make films having a 21 mol % O2 transmission rate of about 150 to about 200 cc/100 in2/24 hr. and hot tack seal initiation temperatures of about 65° C. to 80° C.
-