摘要:
A porous polyimide film has an acid value within a range of 7 mgKOH/g to 20 mgKOH/g determined by acid-base titration, contains a metal group including alkali metals excluding Li, an alkaline earth metals, and silicon at a total content of 100 ppm or less relative to the porous polyimide film, and has a moisture absorption ratio of 0.5% or less.
摘要:
A polyimide precursor solution includes a polyimide precursor having a weight average molecular weight within a range of 20000 to 80000, particles, and an aqueous solvent. The aqueous solvent contains an organic amine compound (A) (excluding a water-soluble organic solvent (B) described below), a water-soluble organic solvent (B) containing at least one selected from the group consisting of N-methyl-2-pyrrolidone, 1,3-dimethyl-2-imidazolidinone, N,N-dimethylformamide, and N,N-dimethylacetamide, and water (C). A content ratio [(A):(B):(C)] of (A), (B), and (C) is within a range of 0.02 to 0.07:0.02 to 0.05:0.88 to 0.96 in terms of mass ratio.
摘要:
An electrostatic charge image developing toner includes a binder resin containing an amorphous polyester resin and a crystalline polyester resin, wherein a ratio of the crystalline polyester resin to a total of the amorphous polyester resin and the crystalline polyester resin is from 12% to 40% by weight, and the toner satisfies the following equations (1) and (2), 30° C.≦T1≦45° C. (1) 1.0×108 Pa≦G′(X)≦5.0×108 Pa (2) wherein T1 represents a temperature at which a storage elastic modulus G′ is 1.0×108 Pa, G′(X) represents a storage elastic modulus G′(B) at a temperature X′° C., and X′° C. represents a temperature at which a ratio of a storage elastic modulus G′(B) to a storage elastic modulus G′(A) has a maximum value.
摘要:
An electrostatic charge image developing toner includes a binder resin and a release agent, and when a peak temperature during a first temperature increase and a peak temperature during a second temperature increase, that are obtained by differential scanning calorimetry including performing the first temperature increase at 10° C./min after holding at 10° C., performing cooling at −10° C./min, performing a heat treatment for 24 hours at 50° C., and performing the second temperature increase at 10° C./min, are represented by Tt1 and Tt2(50° C.), respectively, the following Expression (1) is satisfied: Tt1
摘要:
A porous polyimide film has plural pores, in which an average flattening of the plural pores is within a range of 0.1 to 0.7, a coefficient of variation of a distance between adjacent pores is within a range of 0.10 to 0.40, and a front surface and aback surface communicate with each other through the plural pores.
摘要:
A polyimide precursor solution includes a polyimide precursor, an aqueous solvent containing dimethyl sulfoxide and water, and particles. The content of the dimethyl sulfoxide relative to the particles is within a range of 0.15 to 2.00 in terms of mass ratio.
摘要:
There is provided a porous polyimide film in which the pore distribution width A represented by the following formula is 1.15 or less, the average pore diameter is within a range of 0.50 μm to 3.0 μm, and the air permeation speed is 30 seconds or less: A=(D84/D16)1/2 wherein D16 is the pore diameter at 16% cumulation from the small diameter side of pores, and D84 is the pore diameter at 84% cumulation from the small diameter side of pores.
摘要:
A porous polyimide shaped article has a thickness in a range from 550 μm to 3,000 μm and has a relative dielectric constant of 1.8 or less and a dielectric loss tangent of 0.01 or less at 1 MHz. The porous polyimide shaped article satisfies the following formula: 1.2≤A≤1.6 wherein A represents a square root of a ratio of a pore size D84 where a cumulative percentage by number of pores from smaller sizes is 84% to a pore size D16 where the cumulative percentage by number of the pores from smaller sizes is 16% ((D84/D16)1/2) in a pore size distribution measured by mercury intrusion porosimetry.
摘要:
An electrostatic charge image developing toner includes toner particles containing a binder resin containing a polyester resin forming a sea part and a vinyl resin forming an island part of a sea-island structure, a first release agent existing in the sea part in a domain state, and a second release agent existing in the island part in a domain state, wherein when a cross-sectional area of the second release agent is set to A1 and a cross-sectional area of the first release agent is set to B1 in a cross section of the toner particles, a relationship of 0.2≦A1/B1≦0.8 is satisfied.
摘要:
A polyimide precursor-containing aqueous composition contains at least one polymer material selected from the group consisting of a water-insoluble fibrous organic substance and a polyalkylene oxide having a viscosity-average molecular weight of 5 million or more, a polyimide precursor, particles, and water.