Tape supplying method and tape supplying device

    公开(公告)号:US10087027B2

    公开(公告)日:2018-10-02

    申请号:US14915480

    申请日:2014-09-24

    Applicant: FUJIKURA LTD.

    Abstract: To make a tape length that can be supplied at one time long, and to make it possible to directly supply a tape from a record wound tape.A tape supplying method of this invention includes: connecting a tape end to an outer side of one record wound tape of a first record wound tape and a second record wound tape and a tape end to an inner side of another record wound tape, by matching a surface and a rear surface of the tapes; and after the connecting, supplying a tape of the first record wound tape and the second record wound tape from a tape end of the first record wound tape to an opposite side of a side that has been connected to the second record wound tape.

    BINDER FIBER FOR OPTICAL FIBER UNIT
    2.
    发明申请
    BINDER FIBER FOR OPTICAL FIBER UNIT 审中-公开
    光纤单元用光纤

    公开(公告)号:US20150185428A1

    公开(公告)日:2015-07-02

    申请号:US14419972

    申请日:2013-07-29

    Applicant: FUJIKURA LTD.

    CPC classification number: G02B6/441 G02B1/045 Y10T428/2929

    Abstract: Provided is a binder fiber for an optical fiber unit including a flat sea-island color composite fiber, in which the flat sea-island color composite fiber satisfies the following (1) to (3): (1) a sea component of the flat sea-island color composite fiber has a melting start temperature of 100° C. or higher and a melting peak temperature of 120° C. to 150° C.; (2) the flat sea-island color composite fiber has a width of 0.5 to 3.0 mm and a thickness of 0.15 mm or less; and (3) the flat sea-island color composite fiber has a thermal shrinkage rate of 1.0% or lower after being heated at 100° C. for 3 hours. With the binder fiber, the color developing properties are improved, the shape retaining properties of optical fiber cores are maintained, the optical fiber cores are not compressed, and there is no adhesion with another adjacent binder fiber or the optical fiber cores.

    Abstract translation: 本发明提供一种包含扁平海岛色复合纤维的扁平海岛色复合纤维的光纤单元用粘合纤维,其中,平坦海岛色复合纤维满​​足以下(1)〜(3):(1)扁平海岛色复合纤维的海成分 海岛色复合纤维的熔融开始温度为100℃以上,熔融峰温度为120℃〜150℃。 (2)扁平海岛色复合纤维的宽度为0.5〜3.0mm,厚度为0.15mm以下; (3)扁平海岛色复合纤维在100℃加热3小时后的热收缩率为1.0%以下。 利用粘合纤维,改善了显色性,保持了光纤芯的形状保持性,光纤芯不被压缩,并且与另一个相邻的粘合剂纤维或光纤芯不具有附着力。