Abstract:
A process for the manufacture of single-ply, absorbent paper product, printed on before or after embossing on the Yankee side, air side, or both sides, having a serpentine configuration; low sidedness; a basis weight of at least about 12.5 lbs. per 3000 square foot ream; a specific total tensile strength between 40 and 200 g/3 inches/lb per 3000 square foot ream; a cross direction specific wet tensile strength between 2.75 and 20.0 g/3 inches/lb per 3000 square foot ream; an MD tensile to CD tensile ratio between 1.25 and 2.75; a specific geometric mean tensile stiffness between 0.5 and 3.2 g/inch/% strain per pound per 3000 square foot ream; a friction deviation of less than 0.250; a sidedness parameter of less than 0.30; and a printed sidedness value of nullE of less than 2.