    摘要: A nickel-base alloy is provided having excellent corrosion resistance to both oxidizing and reducing environments in all of the annealed, welded and thermally aged conditions. The alloy has the broad composition:______________________________________ Chromium 12-18 Molybdenum 10-18 Iron 0-3 Tungsten 0-7 Aluminum

    摘要翻译: 在所有的退火,焊接和热老化条件下,提供对氧化和还原环境具有优异的耐腐蚀性的镍基合金。 该合金具有广泛的组成:}铬12-18}钼10-18}铁0-3}钨0-7}铝<0.5}碳0.02最大。 }硅0.08最大 }钴<2}锰<0.5}钛中的一种,高达0.75}钒,锆,钽和铪}镍和偶然的平衡}杂质}

    Cast thermally stable high temperature nickel-base alloys and casting
made therefrom
    2.
    发明授权
    Cast thermally stable high temperature nickel-base alloys and casting made therefrom 失效
    铸造热稳定的高温镍基合金和由其制成的铸件

    公开(公告)号:US4043810A

    公开(公告)日:1977-08-23

    申请号:US644430

    申请日:1975-12-29

    IPC分类号: C22C19/05

    CPC分类号: C22C19/056

    摘要: A cast thermally stable high temperature nickel-base alloy characterized by superior oxidation resistance, sustainable hot strength and retention of ductility on aging is provided by maintaining the alloy chemistry within the composition molybdenum 13.7% to 15.5%; chromium 14.7% to 16.5%; carbon up to 0.1%, lanthanum in an effective amount to provide oxidation resistance up to 0.08%; boron up to 0.015%; manganese 0.3% to 1.0%; silicon 0.2% to 0.8; cobalt up to 2.0%; iron up to 3.0%; tungsten up to 1.0%; copper up to 0.4%; phosphorous up to 0.02%; sulfur up to 0.015%; aluminum 0.1% to 0.5% and the balance nickel while maintaining the Nv number less than 2.31.

    摘要翻译: 通过将组合物中的合金化学维持在13.7%至15.5%之间,提供耐热稳定性优异的耐热性,持久的热强度和延展性对老化的保留性能的铸造热稳定型高温镍基合金; 铬14.7%至16.5%; 碳达0.1%,镧有效量提供高达0.08%的抗氧化性能; 硼至0.015%; 锰0.3%〜1.0%; 硅0.2〜0.8; 钴高达2.0%; 铁达3.0%; 钨高达1.0%; 铜高达0.4%; 磷高达0.02%; 硫至0.015%; 铝0.1%至0.5%,余量为镍,同时保持Nv数小于2.31。

    Thermally stable high-temperature nickel-base alloys
    3.
    发明授权
    Thermally stable high-temperature nickel-base alloys 失效
    耐热稳定的高温镍基合金

    公开(公告)号:US4118223A

    公开(公告)日:1978-10-03

    申请号:US772321

    申请日:1977-02-25

    IPC分类号: C22C19/05

    CPC分类号: C22C19/056

    摘要: A thermally stable, oxidation-resistant nickel-base alloy having good engineering properties for use in mechanical equipment operated at temperatures of up to 1600.degree. F. or higher is provided by maintaining the nickel content above 50% by weight and including as essential elements from about 12 to about 18% chromium, from about 8 to about 18% molybdenum and from about 0.005 to about 0.2% lanthanum by weight. Additional elements may be included in limited amounts provided that the average N.sub.v number of the alloy as defined herein is not substantially above about 2.5 and preferably is below about 2.4.

    摘要翻译: 通过将镍含量保持在50重量%以上,并且包括作为必要元素的含量,提供了具有良好工程性能的热稳定,抗氧化的镍基合金,其用于在高达1600°F或更高的温度下操作的机械设备 约12至约18%的铬,约8至约18%的钼和约0.005至约0.2%的镧。 额外的元素可以以有限的量包括,只要本文所定义的合金的平均Nv数基本上不超过约2.5,优选低于约2.4。

    High chromium nickel base alloys
    4.
    发明授权
    High chromium nickel base alloys 失效
    高铬镍基合金

    公开(公告)号:US4410489A

    公开(公告)日:1983-10-18

    申请号:US284169

    申请日:1981-07-17

    IPC分类号: C22C19/05

    CPC分类号: C22C19/053

    摘要: Disclosed is a nickel-base alloy which provides excellent corrosion resistance to a variety of severe environments, especially hot phosphoric acid. The alloy preferably contains, in weight percent: about 30 chromium, about 4 molybdenum, about 2 tungsten, about 1 Cb/Ta, about 1.5 copper, about 14 iron and the balance nickel plus the impurities and modifying elements usually found in alloy of this class. The alloy is eminently suited for use as articles in chemical processing apparatus in the manufacture and/or containment of phosphoric acid and sulfuric acid.

    摘要翻译: 公开了一种镍基合金,其对各种恶劣环境特别是热磷酸提供优异的耐腐蚀性。 该合金优选以重量百分比计含有:约30铬,约4钼,约2钨,约1Cb / Ta,约1.5铜,约14铁,余量镍加上通常在该合金中发现的杂质和改性元素 类。 该合金特别适用于化学处理设备中制造和/或安装磷酸和硫酸的物品。

    Wear-resistant nickel-base alloy
    5.
    发明授权
    Wear-resistant nickel-base alloy 失效
    耐磨镍基合金

    公开(公告)号:US4191562A

    公开(公告)日:1980-03-04

    申请号:US916340

    申请日:1978-06-19

    IPC分类号: B23K35/30 C22C19/05

    CPC分类号: C22C19/053 B23K35/304

    摘要: Disclosed is a nickel-base alloy typically containing in weight percent, about 2.7 carbon, about 10.5 cobalt, about 27 chromium, about 23 iron, about 10 molybdenum plus tungsten, up to 2.5 maximum tungsten, and the balance nickel and incidental impurities. The alloy is especially suited for use as wear-resistant articles and may be produced in various forms, such as castings, metal powder, tube rod and/or wire and wrought articles. The alloy composition is particularly designed to conserve cobalt and tungsten and yet provide wear-resistant articles comparable to cobalt-base alloys with high tungsten contents.

    摘要翻译: 公开了一种镍基合金,其通常包含重量百分比,约2.7碳,约10.5钴,约27铬,约23铁,约10钼加钨,最多2.5最大钨,余量为镍和附带杂质。 该合金特别适合用作耐磨制品,并且可以以各种形式制造,例如铸件,金属粉末,管棒和/或线和锻造制品。 合金组合物特别设计用于保存钴和钨,并提供与具有高钨含量的钴基合金相当的耐磨制品。