公开(公告)号:US4867852A
公开(公告)日:1989-09-19
申请号:US204262
申请日:1988-06-09
申请人: Fujio Nakao , Nobuyuki Yamamoto , Katumi Anai
发明人: Fujio Nakao , Nobuyuki Yamamoto , Katumi Anai
CPC分类号: D01F11/122
摘要: A method for after-treatment of carbon fiber, which comprises by electrolytic oxidation treatment in an aqueous solution having an ammonium ion concentration of 0.2 to 4.0 mol/l and a pH of at least 7 using the carbon fiber as an anode, followed by treating the resulting fiber in water with an ultrasonic wave of at least 20 kHz frequency at an intensity satisfying the condition: ##EQU1## wherein, F is the frequency (kHz) and T is the treatment period (min) provided that T>0.1.
摘要翻译: 一种碳纤维的后处理方法,其特征在于,使用碳纤维作为阳极,通过在0.2〜4.0mol / l的铵离子浓度和pH为7以上的水溶液中进行电解氧化处理, 所得到的纤维在水中具有至少20kHz频率的超声波,强度满足条件:其中,F是频率(kHz),T是处理周期(min),条件是T> 0.1。