摘要:
The invention concerns novel zeolite Y containing catalyst compositions and the use thereof for the treatment of oxygenated effluents containing nitrogen oxides. The invention further concerns the preparation of such novel zeolite Y containing catalyst compositions.
摘要:
A mixed oxide solid composition of the formulas (I): (a) Mo12Co4.7Bi1Ni2.6Fe3.7W0.5Sn0.5Si1K0.08Ox; (b) Mo12Co3.5Bi1.1Fe0.8W0.5Si1.4K0.05Ox; and (c) Mo12Co3.8Bi1.2Fe0.9W1.1Si1.5K0.05Ox, wherein x is the quantity of oxygen bonded to the other elements and depends on their oxidation states, is suitable for the manufacture of acrolein by oxidizing propylene. The solid composition reacts with propylene according to the redox reaction (1): solidoxidized+propylene→solidreduced+acrolein (1) To manufacture acrolein, gaseous propylene is passed over the solid composition. Redox reaction (1) is conducted at a temperature of 200 to 600° C., at a pressure of 1.01×104 to 1.01 to 106 Pa (0.1 to 10 atmospheres) and with a residence time of 0.01 second to 90 seconds, in the absence of molecular oxygen.
摘要:
A mixed oxide solid composition of formula (I):Mo.sub.12 W.sub.a Bi.sub.b Fe.sub.c Co.sub.d Ni.sub.e Si.sub.f K.sub.g Sn.sub.h O.sub.x (I)where O.ltoreq.a.ltoreq.5, 0.5.ltoreq.b.ltoreq.5, 0.1.ltoreq.c.ltoreq.10, 0.5.ltoreq.d.ltoreq.10, 0.ltoreq.e.ltoreq.10, 0.ltoreq.f.ltoreq.15, 0.ltoreq.g.ltoreq.1, 0.ltoreq.h.ltoreq.2 and x is the quantity of oxygen bonded to the other elements and depends on their oxidation states, is used in the manufacture of acrolein by oxidizing propylene, the solid composition reacting with propylene according to the redox reaction (1):solid.sub.oxidized +propylene.fwdarw.solid.sub.reduced +acrolein(I)To manufacture acrolein, gaseous propylene is passed over a solid composition of formula (I), to conduct the redox reaction (1) by operating at a temperature of 200 to 600.degree. C., at a pressure of 1.01.times.10.sup.4 to 1.01 to 10.sup.6 Pa (0.1 to 10 atmospheres) and with a residence time of 0.01 second to 90 seconds, in the absence of molecular oxygen.
摘要翻译:式(I)的混合氧化物固体组合物:Mo12WaBibFecCodNieSifKgSnhOx(I)其中O = 5,0.5 = b = 5,0.1,c = 10,0.5, d = 10,0 = 10,0 固体还原+丙烯醛(I )为了制备丙烯醛,气态丙烯通过式(I)的固体组合物,通过在200至600℃的温度下操作,在1.01×10 4至1.01至106的压力下进行氧化还原反应(1) Pa(0.1〜10个大气压),停留时间为0.01秒〜90秒,不存在分子氧。