摘要:
The present invention relates to the field of electrode materials, and more specifically, to a carbon-deposited alkali metal oxyanion electrode material as well as to a process for preparing same. More particularly, the process for preparing the carbon-deposited alkali metal oxyanion electrode material comprises a dry milling step of precursors of the alkali metal oxyanion electrode material at an energy sufficient to cause the precursors to agglomerate into strong agglomerates, and a heating step comprising pyrolysis of an organic source to obtain the carbon-deposited alkali metal oxyanion electrode material.
摘要:
The present invention relates to a process for the synthesis of a carbon-deposited alkali metal oxyanion cathode material comprising particles, wherein said particles carry, on at least a portion of the particle surface, carbon deposited by pyrolysis, said process comprising a dry high-energy milling step performed on precursors of said carbon-deposited alkali metal oxyanion prior to a solid-state thermal reaction.
摘要:
A process for preparing an alkali metal oxyanion electrode material having a carbon coating deposited by a thermal treatment, said process comprising a thermal step under a humidified atmosphere of: (i) said alkali metal oxyanion electrode material having a carbon coating deposited by a thermal treatment; (ii) precursors of said alkali metal oxyanion electrode material and an organic precursor of carbon; or (iii) said alkali metal oxyanion electrode material and an organic precursor of carbon, wherein said thermal step is performed at a temperature in the range of about 300° C. to about 950° C.
摘要:
A process for preparing a formulation comprising a carbon-deposited lithium metal phosphate, as precursor of a lithium ion battery electrode coating slurry.
摘要:
Process for improving the electrochemical performance of an alkali metal oxyanion electrode material having a pyrolitic carbon deposit thereon, comprising a heat treatment under a humidified atmosphere where the heat treatment is performed at a temperature in the range of about 300° C. to about 950° C.