OPTICAL GLASS, GLASS MATERIAL FOR PRESS MOLDING, OPTICAL ELEMENT, AND METHOD OF MANUFACTURING SAME
    1.
    发明申请
    OPTICAL GLASS, GLASS MATERIAL FOR PRESS MOLDING, OPTICAL ELEMENT, AND METHOD OF MANUFACTURING SAME 审中-公开
    光学玻璃,用于压制成型的玻璃材料,光学元件及其制造方法

    公开(公告)号:US20130337992A1

    公开(公告)日:2013-12-19

    申请号:US13911473

    申请日:2013-06-06

    CPC classification number: C03C3/062 Y10S501/901

    Abstract: A method of making a press-moldable glass, including melting starting materials, forming a melt, and annealing a formed glass, wherein the melt has a composition such that, (1) when rapidly cooled to room temperature, it becomes glass that has a scattering coefficient of less than 0.005 cm-1 at wavelengths of from 400 to 2,500 nm or comprises crystals with a volumetric ratio of less than 10-6, and (2) when maintained for three hours at a temperature 10° C. higher than the glass transition temperature, maintained for 10 min at a temperature yielding a viscosity of 104.5 to 103.5 dPa·s, and then rapidly cooled to room temperature, (3) the resulting glass has (a) a scattering coefficient of at least one wavelength from 400 to 2,500 nm of greater than 0.01 cm-1 or (b) crystals with a volumetric ratio of greater than 10-5. A temperature for annealing is lower than for glass transition.

    Abstract translation: 一种制造可压制玻璃的方法,包括熔融起始材料,形成熔体并退火成形的玻璃,其中熔体具有如下组成:(1)当快速冷却至室温时,其变为具有 在波长为400至2500nm的散射系数小于0.005cm -1,或包含体积比小于10-6的晶体,和(2)当在比10℃高10℃的温度下保持3小时时 玻璃化转变温度,在104.5〜103.5dPa·s的粘度下保持10分钟,然后迅速冷却至室温,(3)得到的玻璃的(a)至少一个波长的散射系数为400 到2500nm大于0.01cm -1或(b)体积比大于10-5的晶体。 退火温度低于玻璃化转变温度。

Patent Agency Ranking