公开(公告)号:US5552218A
公开(公告)日:1996-09-03
申请号:US360703
申请日:1994-12-21
CPC分类号: D01F6/96 , D01F6/30 , Y10T428/29 , Y10T428/2913 , Y10T428/2967
摘要: The invention relates to polyketone yarns of which the maximum tangential modulus at an elongation of more than 0.2% is at least 10 N/tex which display both high strength and, if so desired, a high elongation at break. The quality number, which is measured on a single filament out of a bundle of at least about 30 filaments spun simultaneously through one spinneret and given as .sigma...epsilon., is higher than 85 mN/tex, preferably higher than 100 mN/tex. The quality number of a yarn spun through one spinneret of one or more holes is higher than 110 mN/tex, preferably higher than 120 mN/tex. The yarns are manufactured by extruding a solution of a linear polymer of alternating ethylene and carbon monoxide units in a resorcinol-containing solvent, after which the solvent is removed with the aid of methanol as coagulant.
摘要翻译: PCT No.PCT / EP93 / 01586 Sec。 371日期1994年12月21日 102(e)1994年12月21日日期PCT 1993年6月21日PCT公布。 出版物WO94 / 00623 日本1994年1月6日本发明涉及聚酮纱线,其伸长率大于0.2%时的最大切向模量为至少10N / tex,其显示出高强度,如果需要,其断裂伸长率高。 质量数量是通过一根喷丝头同时纺丝的一束至少约30根细丝的单根细丝上测量的,并以西格玛的形式给出。 ε高于85mN / tex,优选高于100mN / tex。 通过一个或多个孔的一个喷丝头纺丝的纱线的质量数目高于110mN / tex,优选高于120mN / tex。 通过在含间苯二酚的溶剂中挤出交替的乙烯和一氧化碳单元的线性聚合物的溶液来制造纱线,然后借助于甲醇作为凝结剂除去溶剂。