    摘要: A drive belt has a foundational body made of a polymeric material with elastic properties including a top ply as belt backing and a substructure having a force transmission zone. At least one tensile strand in cord construction is embedded in the drive belt. The tensile strand is completely or partially made of a polyethylene terephthalate (PET), wherein the PET is formed of a yarn associated with the following yarn and cord parameters: a cord linear density of ≦3600 dtex; a yarn hot air thermal shrinkage ≦5% after 2 minutes at 177° C. and at a pre-tension of 0.0005 N/dtex; a corresponding yarn force of ≧3.4 cN/dtex at an elongation of 5% at 25° C. and at a pretension of 0.0005 N/dtex; and a cord hot air thermal shrinking force of ≧0.12 cN/dtex in hot air at 160° C. after 10 minutes and at a pre-tension of 0.0005 N/dtex.

    摘要翻译: 驱动带具有由具有弹性特性的聚合材料制成的基础体,包括顶层作为带背衬和具有力传递区的子结构。 帘线结构中的至少一根拉伸线嵌入驱动带。 拉伸线完全或部分地由聚对苯二甲酸乙二醇酯(PET)制成,其中PET由与以下纱线和绳索参数相关联的纱线形成:帘线线密度为& 3600dtex; 纱线热空气热收缩率n1E; 177℃2分钟后5%,预压力为0.0005N / dtex; 在25℃的伸长率为5%,预压力为0.0005N / dtex的相应的纱线力为≥3cC/ dtex; 10分钟后的160℃的热风和0.0005N / dtex的预张力的帘线热风热收缩力为≧0.12cN / dtex。