摘要: A composite paint for an automotive outer panel comprises an electrodeposition paint film coated on the surface of a steel sheet. The electrodeposition paint film has a minimum melt viscosity not less than 0.2 during hardening and consists essentially of a water paint composition in an amount ranging from 50 to 85 parts by weight upon conversion to a solid content, and a partially cross-linked resin in an amount ranging from 15 to 50 parts by weight upon conversion to a solid content. Additionally, an intermediate paint film is coated on the electrodeposition paint film and has a hardening starting time ranging from 15 to 20 minutes.
摘要翻译: 用于汽车外板的复合涂料包括涂覆在钢板表面上的电沉积漆膜。 电沉积漆膜在硬化期间具有不小于0.2的最低熔体粘度,并且基本上由在固化成分转化率为50至85重量份的量的水漆组合物和基于固体成分的部分交联树脂 的量在转化为固体含量时为15至50重量份。 此外,在电沉积漆膜上涂覆中间漆膜,其硬化开始时间为15〜20分钟。