Oxidation resistant metallic materials
    1.
    发明授权
    Oxidation resistant metallic materials 失效
    耐氧化金属材料

    公开(公告)号:US5800152A

    公开(公告)日:1998-09-01

    申请号:US737993

    申请日:1997-02-14

    摘要: Metallic materials which possess suitable characteristics for serving as an intermediate layer between a thermal barrier coating and a matrix substrate, or as a separator for a solid oxide fuel cell, contain 15 to 40 wt % Cr, 5 to 15 wt % W, 0.01 to 1 wt % M (where M is one or more than two elements chosen from Y, Hf, Ce, La, Nd, and Dy), 0.001 to 0.01 wt % B and a balance of Fe. The average value of the coefficient of thermal expansion of the metallic material is in a range from more than 12.0.times.10.sup.-6 /K to less than 13.0.times.10.sup.-6 /K in a temperature range from room temperature to 1,000.degree. C., and the value is close to that of stabilized zirconia. The metallic materials display excellent high temperature oxidation resistance.

    摘要翻译: PCT No.PCT / JP96 / 00914 Sec。 371日期1997年2月14日 102(e)日期1997年2月14日PCT提交1996年4月3日PCT公布。 公开号WO96 / 31634 日期1996年10月10日具有适合作为隔热涂层和基体基板之间的中间层的特性的金属材料,或作为固体氧化物型燃料电池用隔板,含有15〜40重量%的Cr,5〜15重量% %W,0.01〜1重量%M(其中M为选自Y,Hf,Ce,La,Nd和Dy中的一种或多于两种元素),0.001至0.01重量%B,余量为Fe。 在室温至1000℃的温度范围内,金属材料的热膨胀系数的平均值在大于12.0×10 -6 / K至小于13.0×10 -6 / K的范围内, 值接近稳定氧化锆的值。 金属材料显示出优异的高温抗氧化性。